ABS is a general-purpose thermoplastic polymer. ABS performance characteristics: good rigidity, high impact strength, heat resistance, low temperature resistance, chemical resistance, excellent mechanical strength and electrical properties, easy to process, dimensional stability and surface gloss. ABS becomes one of the preferred plastics for electrical components, home appliances, computers and instrumentation.
PC is high impact strength, good dimensional stability, colorless and transparent, good coloring, electrical insulation, corrosion resistance, wear resistance, but poor self-lubrication. It is easily hydrolyzed at high temperature and has poor compatibility with other resins. Suitable for making small parts, insulated transparent parts and impact resistant parts.
The Rallychem polyester wax structure is very close to the Montan wax, a long non-polar carbon chain with a very strong polar center is able to be compatible with the plastic in the polarity, which is internally lubricated. The part that is incompatible with plastic is used for external lubrication and demoulding. At the same time, it has the both effect of external lubrication and internal lubrication which is the best choice for plastic lubricant.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 691 | Polyester wax | 75 | 1-8 | <3 | 0.96 | Polyester release agent. Low viscosity with non-stick property. | |
RL 925P | Polyester wax | 55 | 50 | <8 | 0.91 | Polyester lubricant. Excellent metal release performance and better gloss. | |
RL 916A | HDOPE wax | 140 | 16 | 9,000@150℃ | <0.5 | 0.98 | Better compatibility to imporve the metal release property. |