Masterbatch consists of a high proportion of pigments, additives and plastic resins. The selected resin has good wetting and dispersing effect on the colorant and is compatible with the pigmented material.
Rallychem wax RL 200 with a high melting point and no odors. It can better wet the surface of the pigment. The excellent pigment coating ability can make the master batch have better color appearance. Less addition will achieve better performance, which has become the best choice to alternate imported PE wax.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 200 | Polyester wax | 114 | – | 700@140℃ | <2 | Excellent pigment wetting and coating, good dispersibility, excellent color appearance, no odor. |
Previous: CPVC Processing