PP melt blown material

MATERIAL SPECIFICATION:

Item      Test Method Specification Testing condition
Melt Mass-Flow Rate(MFR) GB/T 3682 1500 g/10 min 230℃, 2.16kg
Melting point GB/T 19466 165 ℃ 10℃/min
Volatile GB/T 2914 <0.05 % 110℃
Ash GB/T 9345.1 <0.02 % 850℃

APPLICATIONS:

High MFR PP melt-blown material. High barrier properties fabrics could be produced with lower energy consumption

  • Ultra-High MFR
  • Low Volatile
  • Narrow MWD