A coating is a covering that is applied to the surface of an object, usually referred to as the substrate. The purpose of applying the coating may be decorative, functional, or both.

SAMWAX water-based wax emulsions can be compounded with resins to improve the scratch resistance and adhesion of the film. Different wax emulsions also have different gloss levels.

 

Product Component Solid content Melting Range PH value Ionic Character Property
SE 915 HDOPE wax 35% 137 ℃ 5.0-6.0 N Scratch resistant, smoothness feel
SE 913 HDOPE wax 40% 134 ℃ 6.0-7.0 N Excellent wear resistance
SE 737 Carnauba wax 25% 82 ℃ 9.0-11.0 N Antique finishing
SE 773 Carnauba wax 30% 82 ℃ 7.0-10.0 N Scratch resistant, smoothness feel
FT 101 FT wax 40% 100 ℃ 7.5-8.5 N High gloss, better polishability
SD 906 HDOPE wax 50% 137 ℃ 7.0-9.0 N Scratch resistant with matting property
SM 9000 HDOPE wax 50% 137 ℃ 7.0-9.0 N Scratch resistant, smoothness feel
 