Hot melt adhesive is a kind of solid adhesive consisting thermoplastic resin as a main component, combine with plasticizer, antioxidant, flame retardant, wax and filler. Prepared by melt mixing and are non-toxic, no solvent, convenient transportation, storage, fast bonding speed, and high strength, etc.
RALLYCHEM wax has a narrow molecular weight distribution, uniform drop points and good dispersibility. It can be used as a dispersant in the hot melt adhesive industry, effectively improve the heat and cold resistance of hot melt adhesives, good fixability, high bonding strength and excellent acid and alkali resistance.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 616 | Meduim Density OPE wax | 130 | 16 | 700@140℃ | <0.5 | 0.98 | |
RL 100 | Polyester wax | 100 | <0.5 | <3 | 0.92 | Lower melting point and viscosity, good fluidity and good dispersion | |
RL 110 | Polyester wax | 120 | <0.5 | <1 | 0.92 | Higher melting point and viscosity, narrow molecular weight distribution, good fluidity and good dispersion |