High density OPE wax RL-525
For PVC lubricants, Wax emulsions.
.
The RL-525 has lower viscosity and better fluidity. The color of wax emulsion made from RL-525 will be more better.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
25 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 0.5 dmm |
Drop Point, Mettler |
140°C |
Density |
0.99 g/cc |
Viscosity @ 150°C (302°F) |
6,000 cps |
Property |
RL 525 |
Product Form |
Powder |
Size |
100% minus 60 micron
(200 micron, test method 309-OR) |
APPLICATIONS:
PVC Cable filler, TPE process aids, hot melt adhesives, PVC processing, Emulsion