High density OPE wax RL-916
Improve plasticizing speed, super metal stripping and excellent dispersion.
The high density Oxidized PE wax has the property of significantly improving metal release ability, anti-stick and wide processing window while using in U-PVC. The advantages include increasing products homogeneous thus improving the products dimensional stability and productivity. High density oxidized polyethylene wax could use in injection molding applications to improve the strength of weld wires.
Rl-916 unique lubrication and plasticizing effects are not available in other lubricants, and the special component structure is an advantage to reduce the cost of customers. It is often used for PVC products with high requirements for plasticizing, long-term continuous and stable production. Often applied for PVC heat stabilizer, PVC foam products and CPVC products.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
16.5-18 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 0.5 dmm |
Drop Point, Mettler |
140°C |
Density |
0.98 g/cm³ |
Viscosity @ 150°C (302°F) |
15,000 cps |
Property |
RL 916 |
Product Form |
Powder |
Size |
100% minus 60 micron
(200 micron, test method 309-OR) |
Bulk Density |
529 kg/m³ |
APPLICATIONS:
PVC Cable filler(fiberoptics & telecom), TPE process aids, hot melt adhesives, PVC processing
Hot Tags: high density ope wax, manufacturers, suppliers, factory, high quality, price, free samples