High density OPE wax RL-930

It can improve the plasticizing speed and demoulding property of products at high speed, which is suitable for PVC high filling formula.
Product Details
Inquiry
  Material Specification:
Item      Test Method Specification
Acid Number TMP-QCL 29.5-31 mg KOH/g
Property      Value
Hardness @ 25°C (77°F) < 0.5 dmm
Drop Point, Mettler 140°C
Density 0.99 g/cm³
Viscosity @ 150°C (302°F) 25,000 cps
 
Property      RL 930
Product Form Powder
Size 100% minus 60 micron (200 micron, test method 309-OR)
  APPLICATIONS: PVC Cable filler, TPE process aids, hot melt adhesives, PVC processing, Emulsion