Low density OPE wax RL-130A
Acid value 30 easier to be emulsified for wax emulsions.
As a low density oxidized polyethylene wax, RL-130A has an acid value of 30, which makes it easier to be emulsified to make water-based wax emulsion. RL-130A emulsion can be widely used in textile, ink, leather and other industries to play the role of lubrication, scratch and wear resistance.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
28-30 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 5 dmm |
Drop Point, Mettler |
103°C |
Density |
0.94 g/cc |
Property |
RL 130A |
Product Form |
Powder |
Size |
100% minus 40 micron
(200 micron, test method 309-OR) |
Bulk Density |
520 kg/m³ |
APPLICATIONS:
PVC processing, Wax emulsion