Low density OPE wax RL-629TP
Applicable to plastic processing and emulsification, corresponding to imported products.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
14-16 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 5 dmm |
Drop Point, Mettler |
110°C |
Viscosity @ 140°C (284°F) |
170-240 cps |
Density |
0.94 g/cm³ |
Property |
RL 629TP |
Product Form |
Powder |
Size |
100% minus 60 micron(200 micron, test method 309-OR) |
APPLICATIONS:
PVC stabilizers, PVC processing, CPVC processing, Wax emulsion, Engineering Plastic