Low density OPE wax RL-6882
Mildly improve the plasticizing speed, anti precipitation and improve the surface brightness of PVC products.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
9.5-11 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
<5 dmm |
Drop Point, Mettler |
110°C |
Density |
0.94 g/cm3 |
Viscosity @140°C (284°F) |
20 cps |
Property |
RL 6882 |
Product Form |
Powder |
Size |
100% minus 60 micron
(200 micron, test method 309-OR) |
APPLICATIONS:
PVC stabilizers, PVC processing, CPVC processing, Wax emulsion, Engineering Plastic
Hot Tags: Low density OPE wax, manufacturers, suppliers, factory, high quality, price, free samples