Polyethylene wax RL-100
Lower melting point and viscosity, effective delayed plasticization.
As PVC external lubricant. Lower melting point and viscosity, effective delayed plasticization, and excellent release properties.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
< 0.5 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 3 dmm |
Drop Point, Mettler |
100°C |
Density |
0.92 g/cc |
Property |
RL 100 |
Product Form |
Powder |
Size |
100% minus 60 micron
(200 micron, test method 309-OR) |
APPLICATIONS:
PVC processing