In the process of producing color masterbatch and modified plastics, the FT wax is helpful for the dispersion and excellent smoothness of fillers. Can be used as PVC external lubricant, low viscosity can improve the production speed of products.
Rl-001 is a special FT wax refined by RALLYCHWM with a unique process. Extremely narrow molecular weight distribution, suitable for PVC, CPVC, hot melt adhesive and other industries. Countertype of SARAWAX SX - 105.
Material Specification:
Item | Test Method | Specification |
Acid Number | TMP-QCL | <1 mg KOH/g |
Property | Value | |
Hardness @ 25°C (77°F) | < 1 dmm | |
Drop Point, Mettler | 115°C | |
Density | 0.92 g/cc |
Property | RL 001 |
Product Form | Powder |
Size | 100% minus 60 micron (200 micron, test method 309-OR) |
Bulk Density | 510 kg/m³ |
APPLICATIONS: PVC, CPVC processing, Hot melt adhesive