RL-907A is a high viscosity, low acid oxidized polyethylene wax, very effective for accelerating plasticization and reducing the gloss of profiles.
Material Specification:
Item |
Test Method |
Specification |
Acid Number |
TMP-QCL |
7-8.5 mg KOH/g |
Property |
Value |
Hardness @ 25°C (77°F) |
< 0.5 dmm |
Drop Point, Mettler |
140°C |
Density |
0.99 g/cm³ |
Viscosity @ 150°C (302°F) |
27,000 cps |
Property |
RL 907A |
Product Form |
Powder |
Size |
100% minus 60 micron
(200 micron, test method 309-OR) |
APPLICATIONS:
PVC processing, ABS, PC injection