Low density OPE wax RL-9308

Mildly improve the plasticizing speed, anti precipitation and improve the surface brightness of PVC products. It is suitable for PVC processing.
Product Details
Inquiry
  Material Specification:
Item      Test Method Specification
Acid Number TMP-QCL 10 mg KOH/g
Property      Value
Hardness @ 25°C (77°F) < 5 dmm
Drop Point, Mettler 110°C
Viscosity @ 140°C (284°F) 160 cps
Density 0.94 g/cm³
 
Property      RL 9308
Product Form Powder
Size 100% minus 60 micron (200 micron, test method 309-OR)
  APPLICATIONS: PVC stabilizers, PVC processing, CPVC processing, Wax emulsion  