Polyester wax RL-70

PVC calendering external lubricant, improve demoulding, excellent surface effect, suitable for transparent products.
Product Details
Inquiry
  Material Specification:
Item      Test Method Specification
Acid Number TMP-QCL 5-20 mg KOH/g
Property      Value
Drop Point, Mettler 56-62°C
Density 0.91 g/cm³
Saponification Value 240-270 mg KOH/g
 
Property      RL 70
Product Form Powder
Size 100% minus 60 micron (200 micron, test method 309-OR)
PVC calendering exernal lubricant. Good compatibility and does not precipitate. It can reduce the frequency of wiping roller and extend the machine running time. Suitable for high transparent products. APPLICATIONS: PVC calendering external lubricant  

Hot Tags: high molecular weight polyester wax, manufacturers, suppliers, factory, high quality, price, free samples