PVC edge banding is a material that protects, decorates and beautifies the section of furniture sheet. It can make a piece of furniture show the overall effect of clear and colorful wood grain.
In the production of PVC edge banding, the required lubricant must be adapted to the high-speed extrusion production process to ensure smooth processing and the wax can not be precipitated to affect the later processing. RALLYCHEM’s range of lubrication products can effectively help customers improve product quality and reduce rejects rate.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 11 | Polyester wax | 76 | 1-3 | <5 | 0.91 | Internal lubricant. Good PVC compatibility provides excellent high fluid flow and reduced PVC intermolecular friction. | |
RL 61 | Polyester wax | 70 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent PVC compatibility without precipitation. Applicable to PVC transparent products, improve fluidity and dispersion. | |
RL 60 | Polyester wax | 55 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent compatibility and dispersibility for high transparency requirements, improved process flow and non-stick properties. | |
RL 100 | Polyester wax | 100 | <0.5 | <3 | 0.92 | External lubricant. Lower melting point and viscosity, effective delayed plasticization, and excellent release properties. | |
RL 117 | Polyester wax | 118 | – | 300@150℃ | <2 | External lubricant. High drop point and viscosity, good plasticization control and dispersion properties, and maintains dimensional stability of the product. | |
RL 200 | Polyester wax | 118 | – | 1,000@150℃ | <2 | External lubricant. Higher drop point and viscosity, good plasticization control and dispersion properties, excellent release effect and better surface gloss. | |
RL 016A | LDOPE wax | 110 | 16 | <2 | 0.91 | Excellent external lubricity and fluidity, better surface gloss. | |
RL 925 | HDOPE wax | 140 | 25 | 10,000@150℃ | <0.5 | 0.99 | Fast increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties. |
RL 916A | HDOPE wax | 140 | 16 | 9,000@150℃ | <0.5 | 0.98 | Improve PVC plasticizing speed, superior metal peelability and excellent dispersion properties. |