Foam Board is a lightweight rigid material used primarily in the manufacture of signs and displays. It is considered robust for outdoor use, being immune to rain and resistant to wind and sunlight.

Rallychem’s oxidized polyethylene wax products help customers achieve superior plastic control and metal stripping. The external lubricant can effectively help the product to be demolded and get a smooth surface and high gloss. The highly dispersible internal lubricant helps to reduce the viscosity of the material, increase fluidity and have a wider processing window.

 

Product Form Drop point(℃) Acid Number (mg KOH/g) Viscosity (cps) Hardness (dmm) Density (g/cc) Property
RL 11 Polyester wax 76 1-3 <5 0.91 Internal lubricant. Good PVC compatibility provides excellent high fluid flow and reduced PVC intermolecular friction.
Suitable for PVC advertising board / cabinet board / floor.
RL 61 Polyester wax 70 1-3 <8 0.91 Internal lubricant. Excellent PVC compatibility without precipitation. Applicable to PVC transparent products, improve fluidity and dispersion.
Suitable for PVC advertising board / cabinet board / floor.
RL 100 Polyester wax 100 <0.5 <3 0.92 External lubricant. Lower melting point and viscosity, effective delayed plasticization, and excellent release properties.
Suitable for PVC advertising board / cabinet board / floor.
RL 117 Polyester wax 118 300@150℃ <2 External lubricant. High drop point and viscosity, good plasticization control and dispersion properties, and maintains dimensional stability of the product.
Suitable for PVC advertising board / cabinet board / floor.
RL 200 Polyester wax 118 1,000@150℃ <2 External lubricant. Higher drop point and viscosity, good plasticization control and dispersion properties, excellent release effect and better surface gloss.
Suitable for PVC advertising board / cabinet board / floor.
RL 916 HDOPE wax 140 16 14,000@150℃ <0.5 0.98 Effectively improve the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties.
Suitable for PVC advertising board / cabinet board.
RL 925 HDOPE wax 140 25 10,000@150℃ <0.5 0.99 Fast increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties.
Suitable for PVC advertising board / cabinet board / floor.
RL 930 HDOPE wax 140 30 25,000@180℃ <0.5 0.99 Faster increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties.
Suitable for high filled formula PVC  cabinet board / floor.
RL 825 HDOPE wax 140 25 10,000@150℃ <0.5 0.99 Fast increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties.
Suitable for PVC advertising board / cabinet board / floor.
RL 525 HDOPE wax 140 25 6,000@150℃ <0.5 0.99 Fast increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties.
Suitable for PVC advertising board / cabinet board / floor.
 