As a wide and popular construction and decoration material, PVC profiles/pipes have excellent characteristics such as strong corrosion resistance, easy adhesion, low price and hard texture.
Rallychem PVC lubricants can increase production efficiency and finished goods rate, and reduce the risk of precipitation. The excellent lubricity would help the PVC pipe/profile get better surface, and good fluidity can also decrease the complex shape profile process difficulty.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 11 | Polyester wax | 76 | 1-3 | <5 | 0.91 | Internal lubricant. Good PVC compatibility provides excellent high fluid flow and reduced PVC intermolecular friction. | |
RL 61 | Polyester wax | 70 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent PVC compatibility without precipitation. Applicable to PVC transparent products, improve fluidity and dispersion. | |
RL 60 | Polyester wax | 55 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent compatibility and dispersibility for high transparency requirements, improved process flow and non-stick properties. | |
RL 100 | Polyester wax | 100 | <0.5 | <3 | 0.92 | External lubricant. Lower melting point and viscosity, effective delayed plasticization, and excellent release properties. | |
RL 117 | Polyester wax | 118 | – | 300@150℃ | <2 | External lubricant. High drop point and viscosity, good plasticization control and dispersion properties, and maintains dimensional stability of the product. | |
RL 200 | Polyester wax | 118 | – | 1,000@150℃ | <2 | External lubricant. Higher drop point and viscosity, good plasticization control and dispersion properties, excellent release effect and better surface gloss. | |
RL 016A | LDOPE wax | 110 | 16 | <2 | 0.91 | Excellent external lubricity and fluidity, better surface gloss. | |
RL 925 | HDOPE wax | 140 | 25 | 10,000@150℃ | <0.5 | 0.99 | Fast increase the plasticizing speed of PVC, superior metal stripping and excellent dispersion properties. |
RL 916A | HDOPE wax | 140 | 16 | 9,000@150℃ | <0.5 | 0.98 | Improve PVC plasticizing speed, superior metal peelability and excellent dispersion properties. |