PVC transparent products are widely used in medical materials, decorative films, shrink films, crystal cloth and other industries. It is often produced by processes like blow molding, extrusion, and calendering.
The requirements of the PVC transparent product lubricants are more strict than other kinds PVC product. Normally the general lubricant will affect the transparency of the product, but the RL916A not only will not affect the transparency with proper addition, but also help the product to be better demolded. In the PVC film product process, the RL916A is already an essential additive in the formulation.
Product | Form | Drop point(℃) | Acid Number (mg KOH/g) | Viscosity (cps) | Hardness (dmm) | Density (g/cc) | Property |
RL 11 | Polyester wax | 76 | 1-3 | <5 | 0.91 | Internal lubricant. Good PVC compatibility provides excellent high fluid flow and reduced PVC intermolecular friction. | |
RL 61 | Polyester wax | 70 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent PVC compatibility without precipitation. Applicable to PVC transparent products, improve fluidity and dispersion. | |
RL 60 | Polyester wax | 55 | 1-3 | <8 | 0.91 | Internal lubricant. Excellent compatibility and dispersibility for high transparency requirements, improved process flow and non-stick properties. | |
RL 07A | Polyester wax | 55 | 1-10 | <8 | 0.91 | PVC calendering exernal lubricant. Good compatibility and does not precipitate. It can reduce the frequency of wiping roller and extend the machine running time. | |
RL 70 | Polyester wax | 55 | 1-10 | <8 | 0.91 | PVC calendering exernal lubricant. Good compatibility and does not precipitate. It can reduce the frequency of wiping roller and extend the machine running time. Suitable for high transparent products | |
RL 916A | HDOPE wax | 140 | 16 | 9,000@150℃ | <0.5 | 0.98 | Excellent metal stripping and effective promotion of plasticization, especially suitable for PVC shrink film and blown film, it is already an essential additive in the formulation. |
RL 016A | LDOPE wax | 110 | 16 | <2 | 0.91 | Excellent external lubricity and fluidity, better surface gloss. |