A textile is a flexible material consisting of a network of natural or artificial fibres (yarn or thread). Textiles are formed by weaving, knitting, crocheting, knotting, or felting.

SAMWAX wax emulsion has excellent emulsion stability. Well compatible with anionic, cationic finishing resins and is able to use in combination with acids, metal salts, amines, dye fixing agents and other textile auxiliaries. SAMWAX wax emulsions can be finished by padding and impregnating machines and appliable in slurry spinning machine, air jet finishing machines, twisting machine, winder, sizing machine, warping machine, slot machine, shaker and so on.

 

Product Component Solid content Melting Range PH value Ionic Character Property
SE 910 HDOPE wax 35% 137 ℃ 7 N Yarn lubrication, smoothness feeling
SE 915 HDOPE wax 35% 137 ℃ 5.0-6.0 N For fabric finishing and printing paste
SE 937 HDOPE wax 35% 137 ℃ 5.0-6.0 C Good yarn lubrication performance and low yellowing, can be used for anti-needle hole and non-ironing
SE 938 HDOPE wax 35% 120 ℃ 5.0-6.0 C Excellent yarn lubrication, strong protection and needle hole prevention
SE 947 HDOPE wax 30% 115 ℃ 5.0-6.0 C Good stability and hydrophilicity, no volatilization
SE 331 Paraffin wax 50% 58℃ 6.5-7.5 N Yarn lubricating, excellent stability
 