What does the acid value of oxidized polyethylene wax represent in PVC processing?

Oxidized polyethylene waxes are used as both internal and external PVC lubricants. There are a number of common models on the market, such as 916, 925 and 930, which represent acid value 16, acid value 25 and acid value 30, respectively.
Generally speaking, the acid value represents the polarity of the oxidized wax and is positively correlated. The higher the acid value, the higher the polarity of the oxidized wax. In practical PVC processing, a higher acid value means that the oxidized wax has a more pronounced internal lubrication effect and increases the speed of plasticization. For example, the plasticizing speed of 930 with acid value 30 is significantly faster than that of 916 with acid value 16, so it is more suitable for PVC products with higher plasticizing requirements, such as SPC flooring, stone wall panels and other highly filled products.

On the other hand, when the acid value of oxidized polyethylene wax is higher, it is more in favor of internal lubrication, and its external lubrication effect will be relatively weakened. Therefore, oxidized polyethylene waxes with low acid values are more suitable for PVC products with high demands on post-molding and surface. For example, shrink films, calendered sheets, etc.


Therefore, 916A with an acid value of 16 can be used as a good late release agent after plasticization has reached the required level.
İlginizi Çekebilir
Rallychem Showcased at the 34th Plast Eurasia Istanbul, Co‑creating a Greener Future with the World
2025 / 12 / 08
Why Your Coatings Perform Better with Polyethylene Wax Additives?
2025 / 11 / 19
Why Polyethylene Wax Is the Key to High Performance Printing Inks
2025 / 11 / 18
[Exhibition Invitation] RALLYCHEM · Sincerely Invites You to Attend CHINACOAT 2025
2025 / 11 / 14
[Exhibition Invitation] Countdown to Plastics & Rubber Indonesia 2025 – RALLYCHEM Looks Forward to Meeting You
2025 / 11 / 07

Sorularınız İçin Lütfen Arayınız
Rallychem Size Yardımcı Olmaktan Mutluluk Duyacaktır!

+86 13456396233