Material Specification:
Item |
Specification |
Form |
Light Gray Liquid |
Technical Data |
Wax Type |
Carnauba Wax |
Solids Content |
25±1% |
Ionic Character |
Non ionic |
Melting Range |
82℃ |
pH-Value PH |
9.0-11.0 |
Storage:
To be stored at least 12 months under +6-28℃, to avoid frozen and temperature higher than 40℃
Dosage:
0.5-3% in reference to impregnation method of textile industry
Packaging:
* 50 KG/Drum
* 120 KG/Drum
* 1000 KG/Drum