* Paint (flooring, furniture): high gloss and high feeling * Improve performance of printing ink, leather finishing agent, varnish, aqueous varnish * Gloss, slip, scratch/ wear/ abrasion/ impact/ stain resistance   Material Specification:
Item Specification
Form Light Yellow Liquid
Technical Data
Wax Type PE Wax
Solids Content 33-35%
Ionic Character Non ionic
Melting Range 137℃
pH-Value PH 7.0
Particle size 20 nm
  Storage To be stored at least 12 months under +6-28℃, to avoid frozen and temperature higher than 40℃   Dosage 4-10% in reference to the entire formulation   Packaging * 50 KG/Drum * 120 KG/Drum * 1000 KG/Drum  