PVC pipes, conduits, and profiles are processed at temperatures high enough to trigger thermal degradation. That’s why heat stabilizers are non‑optional in PVC processing: they protect the polymer during extrusion and help maintain long-term performance.
But in real production, “stabilization” is not only about chemistry. A stabilizer package must also deliver processing stability, metal release, and clean surface quality—and this is where wax additives (lubricant waxes) play a critical role.
When PVC is heated during extrusion (commonly ~160–200°C depending on formulation and equipment), it can undergo dehydrochlorination (release of HCl). If not controlled, it causes:
For pipe and conduit applications, stabilizers help processors maintain:
Most commercial PVC stabilizer packages are designed as multi-component systems. Besides the stabilizer actives, they often include co-stabilizers and lubricants—and waxes are widely used because they can strongly influence the processing window.
Properly selected wax additives can help:
In rigid PVC, processors typically need a balanced internal/external lubrication profile:
Wax chemistry (molecular weight, melting/softening point, polarity) influences where a wax sits on this spectrum. An imbalanced system may show:
Depending on the stabilizer system and the target product, wax additives may include:
Selection should be based on: fusion window, torque curve, melt pressure stability, die cleanliness, surface finish, and downstream requirements.
Rallychem’s lubricants are the perfect match for PVC heat stabilizers.
We offer high-performance and cost-effective lubricants, as well as customized functional targeting lubricants to better fit the producer’s specific stabilization system. Whether for highly filled PVC or PVC transparent products, RALLYCHEM can help achieve a wider processing window.
Key Benefits of Rallychem Wax Additives:
1 Enhanced Stability: Improves both dynamic and static stability of stabilizers, obtaining better whiteness.
2 Wider Processing Window: Reduces the risk of degradation during temperature fluctuations.
3 Plate-out Control: Effectively reduces precipitation and die build-up.
4 Superior Surface Finish: Improves mold release for an excellent surface effect.
5 Consistency: Delivers good batch-to-batch stability for reliable production.
قد تكون مهتمًا
New Product Teaser|Entering the Era of “Stability Competition” in Engineering Plastics, a True Montan Wax Replacement Solution Has Arrived
2026 / 04 / 20
Rallychem Advanced Materials ── From Material Behavior to Process-Controlled Performance
2026 / 04 / 16
شمع البولي إيثيلين البولي إيثيلين المؤكسد مقابل شمع البولي إيثيلين المؤكسد: مقارنة أداء التشحيم في معالجة أنابيب PVC
2026 / 04 / 06
لماذا تحتاج اللدائن الهندسية إلى “شمع خاص”؟ مقدمة فنية عن شمع البوليستر الاصطناعي Rallychem
2026 / 04 / 02
دليل تزييت وتقوية أنابيب PVC: تحقيق التوازن المثالي بين التكلفة والأداء من أجل بثق فعال ومستقر
2026 / 03 / 19