Knowing is not only important, it is also important to know why. Understanding the microscopic location of PE waxes and oxidized polyethylene waxes helps us to understand the lubrication principle more intuitively and scientifically, so that we can optimize our formulations to produce better PVC products.

According to a study by the University of South Africa, by using a scanning electron microscope, it is possible to observe the microscopic behavior of PE wax in the actual processing of PVC. We can see that the gray is PVC particles and the red is polyethylene wax. The non-polar polyethylene wax cannot combine with the PVC particles due to its incompatibility with PVC. It mainly acts between the particles of PVC. It plays the role of external lubrication that delays plasticization and avoids PVC resin sticking to metal screws and barrels.
Fischer-Tropsch wax behaves similarly to PE wax in that it acts as an external lubricant.

The oxidized polyethylene wax, on the other hand, carries a polarity that enables it to combine with the PVC resin. Through the scanning electron microscope, we can find that compared with PE wax, oxidized wax is able to coat each PVC particle better, which is equivalent to putting on a lubricating coat for each PVC particle precisely. Therefore, during processing, no matter how the screw is sheared, there is no loss of lubricating properties and the release of mold is guaranteed at the late stage of processing; the internal lubrication of oxidized polyethylene waxes also promotes plasticization, which improves the processing efficiency and increases the daily production volume of the factory; and in the case of PVC products filled with high-calcium powder, the
In the case of high calcium filled PVC products, the oxidized polyethylene wax provides better protection for the screw, thus prolonging the screw’s service life.
قد تكون مهتمًا
New Product Teaser|Entering the Era of “Stability Competition” in Engineering Plastics, a True Montan Wax Replacement Solution Has Arrived
2026 / 04 / 20
Rallychem Advanced Materials ── From Material Behavior to Process-Controlled Performance
2026 / 04 / 16
شمع البولي إيثيلين البولي إيثيلين المؤكسد مقابل شمع البولي إيثيلين المؤكسد: مقارنة أداء التشحيم في معالجة أنابيب PVC
2026 / 04 / 06
لماذا تحتاج اللدائن الهندسية إلى “شمع خاص”؟ مقدمة فنية عن شمع البوليستر الاصطناعي Rallychem
2026 / 04 / 02
دليل تزييت وتقوية أنابيب PVC: تحقيق التوازن المثالي بين التكلفة والأداء من أجل بثق فعال ومستقر
2026 / 03 / 19