Verbesserung von PVC-U-Rohren - die Rohre werden für die landwirtschaftliche Bewässerung verwendet
The original formula: made the production batches unstable, resulting in low efficiency and increased costs.
Low toughness agent efficiency: resulting in insufficient toughness
1、Continuous Lubrication Protection
Provides consistent lubrication during the entire processing cycle (beginning, middle, and end).
2、Superior Anti-Precipitation Performance
Better resistance to precipitation compared to traditional formulations.
3、Reduce the cost
Polyester Homopolymer enable the manufacturer to add in more CaCO3 without losing the property.
4、Wider Processing Range
Reduces the frequency of degradation and provides more stable processing conditions.
5、Superior Shear Resistance
Better shear resistance compared to traditional formulations, allowing for the addition of more calcium carbonate.
6、Suitable for Large Diameters
Can be effectively used for large diameter pipes(Dn200/315/630).
RALLYCHEM’s formulation increases the toughening efficiency, resulting in significantly improved product durability, and reduce the cost via adding more CaCO3.