Spezifische Lösungen für das Problem der Sprödigkeit von PVC-Rohren bei niedrigen Temperaturen
PVC tends to exhibit brittleness, insufficient toughness, and poor compressive performance in winter, which has always troubled our customers.

We inspect our customers’ equipment and process conditions, and take some formula samples for testing in the Rallychem Chemicals laboratory to identify the cause of the issues.

Rallychem Chemicals has customized two sets of solutions, and technical service personnel, carrying the customized plans, conduct on-site production tests for customers.

Both formulations have been tested, and after the application of polyester wax and polyester homopolymer products, the performance of the customer’s pipe materials has been significantly enhanced without increasing production costs. In terms of compression resistance, cold impact, and hand bending tests, the performance is superior to the pipes produced with the customer’s original formula. During the production process, the transition in the process is smooth, and the current is more stable.
The processing range of polyester wax is superior to the traditional combination of stearic acid and PE wax for both internal and external applications, and there is further room for optimization in production speed.
Verwandte Fälle

PVC-Schrumpffolienlösung

Verbesserung von PVC-U-Rohren - die Rohre werden für die landwirtschaftliche Bewässerung verwendet

Lösung für die Anwendung von PVC-Elektroinstallationsrohren

Herausforderungen bei PVC-Schaumplatten

Lösung für den Bruch von PVC-Kohlenstoff-Kristallplatten

SPC Floor Resilience Enhancement Solution