2025 / 07 / 04
Why does PVC turn yellow? You may never have understood these 3 situations systematically
Anyone working with PVC knows that yellowing is a major problem that cannot be avoided.
Yellowing of pipes, dirtiness of sheets, graying of cables…not only affects appearance but can also impair performance.
But do you know why PVC yellows? And how can it be effectively prevented?
Today, we’ll provide a comprehensive analysis of the yellowing mechanism, prevention and control measures, and testing methods.
▶ Root cause: High-temperature processing and repeated heating break C-Cl bonds, generating HCl and forming a conjugated polyene structure (a chain of conjugated double bonds).
▶ Color development mechanism: The more conjugated double bonds there are, the stronger the π electron’s light absorption ability, causing the color to deepen from light yellow to orange-yellow to brown-red.
▶ Detection method: UV-Vis absorption spectroscopy: Detect the absorption peak between 250-450nm. Colorimeter: The higher the yellowing index Δb*, the darker the color.

▶ Reaction mechanism:
▶ Accelerated photooxidation: Chain reaction of reactive oxygen species (·O, ROOH) in the high-energy UV-A/B bands of UV light
▶ Cause:
▶ Additional Note: Some low-molecular-weight HALS are also susceptible to decomposition, especially in the presence of acidic substances (such as stearic acid), causing them to discolor more easily.
| Yellowing Types | Key Prevention Measures |
|---|---|
| Conjugated Double Bond Yellowing | Heat Stabilizer + Epoxy Compound + Temperature Control≤180°C |
| Oxidative Yellowing | Primary/Secondary Antioxidants + UV Absorbers + Titanium Dioxide/Coating Shielding |
| Yellowing Caused by Nitrogen-Containing Additives | Using Polymer HALS + Nitrogen-Free Alternatives + Metal Passivators |
PVC yellowing is a “chemical storm” caused by the combined effects of heat, light, and oxygen. To truly control it, we can’t rely solely on a single additive. Instead, we must develop a multi-faceted closed-loop approach encompassing formulation design, additive selection, processing control, and testing mechanisms. Only in this way can we achieve long-term anti-yellowing and stable appearance quality.
Quizá le interese
RALLYCHEM brilla en la K 2025 de Düsseldorf | ¡Gracias por acompañarnos!
2025 / 10 / 17
Octubre en Düsseldorf - Nos vemos en K 2025
2025 / 09 / 30
Rallychem asistió a la reunión anual de la Asociación de Tuberías de Plástico de China y a la Conferencia de Intercambio Industrial
2025 / 08 / 29
¿Se rompe el cartón con frecuencia? Controle su extrusora en tres pasos para eliminar la fragilidad del cartón de espuma de PVC.
2025 / 08 / 22
Una nueva opción para la lubricación interna de placas de cristal de carbono | Cera de poliéster RL-1116F, una solución profesional con precio estable y alta eficacia
2025 / 08 / 15