Why is it so difficult to reach 60% chlorine content in CPVC pipe and dry mix?
Why did the national standard lower the chlorine content of CPVC pipe and dry mix from 60% to 55%?
Why is it so difficult to reach 60% chlorine content in CPVC?

Selection of high-quality raw materials: liquid-phase CPVC resin chlorine content is usually between 64% and 67%, which is more common. Solid-phase CPVC resin chlorine content can be more than 68%, but the color control is more difficult.
Application of efficient additives: Choose additives with small amount and high efficiency to reduce the dilution of chlorine content.
Innovative formulation ideas: Abandon the traditional PVC formulation mode, reduce the use of non-essential ingredients under the premise of ensuring processing convenience, so as to improve the overall chlorine content level.

Rallychem Chemical’s polyester wax and polyester homopolymer formulations are highly effective additives for CPVC production, providing excellent performance at lower usage levels, thereby reducing costs.
The use of polyester waxes and polyester homopolymers stabilizes the chlorine content of CPVC products at 58-59%, approaching 60%. In addition, we provide one-stop service to help customers reduce the need for production testing and adjustments, and provide them with efficient and economical production formulations and solutions.


Quizá le interese
How Polyethylene Wax Enhances Pigment Dispersion and Color Consistency in Masterbatch Production
2026 / 02 / 05
Cost Optimization in PVC Processing: Using Targeted Polyester Wax to Partially Replace Stearic Acid and Paraffin Wax
2026 / 02 / 04
Lubricación de plásticos de ingeniería: Por qué la cera de poliéster es la alternativa a la cera Montan
2026 / 01 / 23
Optimización de la durabilidad del revestimiento con los aditivos de cera avanzados de RallyChem
2026 / 01 / 22
¿Qué es el lubricante de PVC y por qué es esencial en la transformación del PVC?
2025 / 12 / 31