    نرم‌کننده پلاستیک مایع EP

  • Model

    آر ال ۵۰۱

  • Industry & Functionality

    PVC products

    reduces the probability of scorching during the production and helps to improve the yield.

  • Specifications

    50 KG/Drum
    120 KG/Drum
    1000 KG/Drum
  • Acid value

    1.8 mg KOH/g

  • Volatile

    0.6 %,105℃

  • TDS/MSDS:

    TDS MSDS

You can send requirements and suggestions to us.

We value your requirements and recommendations very much. If you have any questions concerning our services, don't hesitate to ask. Our knowledgeable Rallychem engineers are happy to assist you!

* Company Name

* Name

Phone

* E-Mail

* From which industry

Other Industry Applications باتری لیتیومی انرژی نو فرآوری فلزات میوه‌ها/دانه‌ها علامت‌گذاری با چسب حرارتی اصلاح آسفالت Adhesives Coating and Ink Auxiliaries Textile Auxiliaries اصلاح پلاستیک مهندسی Color and Filler Masterbatches پردازش CPVC پردازش پی‌وی‌سی

What you need

واتس‌اپ

برای استعلام لطفاً تماس بگیرید

رالی‌کم با کمال میل به شما کمک خواهد کرد!

+86 13456396233