• Informations sur le produit

  • Données techniques

  • Type de cire

    Cire PE

  • Modèle

    SE-331

  • Industrie et fonctionnalité

    Varnish

    a great water-based brightener in paper and film packaging

    Water-based adhesives

    suitable for the preparation of water-based adhesives,especially suitable for packaging film (BOPP film, PE film, etc.) and paper sealing glue

    Polyurethane coating

    improve the anti-friction ability of waterborne polyurethane coatings, such as parquet sealants

    Printing ink

    improve the anti-friction ability of water-based printing ink

    Textile

    improve the sewing, anti-friction and tear strength of fabric

    Floor Polishes

    strengthen hardness and toughness of floor surface, improve its service life

    High compatibility

    High compatibility to polymer dispersion, resin solution, plasticizer, film forming agent

  • Spécifications

    50 KG/tambour
    120 KG/tambour
    1000 KG/tambour

Vous pouvez nous faire part de vos besoins et de vos suggestions.

Nous accordons une grande importance à vos exigences et à vos recommandations. Si vous avez des questions concernant nos services, n'hésitez pas à nous les poser. Nos ingénieurs Rallychem compétents se feront un plaisir de vous aider !

* Nom de l'entreprise

* Nom

Téléphone

* Courrier électronique

* De quel secteur s'agit-il ?

Autres applications industrielles Piles au lithium à énergie nouvelle Traitement des métaux Fruits/graines Marquage à chaud Modification de l'asphalte Adhésifs Auxiliaires d'enduction et d'encrage Auxiliaires textiles Ingénierie de la modification des matières plastiques Mélanges maîtres de couleurs et de charges Traitement du CPVC Traitement du PVC

Ce dont vous avez besoin

WhatsApp

Pour toute demande de renseignements, veuillez appeler

Rallychem se fera un plaisir de vous aider !

+86 13456396233