Why is it so difficult to reach 60% chlorine content in CPVC pipe and dry mix?
Why did the national standard lower the chlorine content of CPVC pipe and dry mix from 60% to 55%?
Why is it so difficult to reach 60% chlorine content in CPVC?

Selection of high-quality raw materials: liquid-phase CPVC resin chlorine content is usually between 64% and 67%, which is more common. Solid-phase CPVC resin chlorine content can be more than 68%, but the color control is more difficult.
Application of efficient additives: Choose additives with small amount and high efficiency to reduce the dilution of chlorine content.
Innovative formulation ideas: Abandon the traditional PVC formulation mode, reduce the use of non-essential ingredients under the premise of ensuring processing convenience, so as to improve the overall chlorine content level.

Rallychem Chemical’s polyester wax and polyester homopolymer formulations are highly effective additives for CPVC production, providing excellent performance at lower usage levels, thereby reducing costs.
The use of polyester waxes and polyester homopolymers stabilizes the chlorine content of CPVC products at 58-59%, approaching 60%. In addition, we provide one-stop service to help customers reduce the need for production testing and adjustments, and provide them with efficient and economical production formulations and solutions.


Vous pouvez être intéressé
Engineering Plastics Lubrication: Why Polyester Wax is the Montan Wax Alternative
2026 / 01 / 23
Optimisation de la durabilité des revêtements avec les additifs de cire avancés de RallyChem
2026 / 01 / 22
Qu'est-ce qu'un lubrifiant pour PVC et pourquoi est-il essentiel dans la transformation du PVC ?
2025 / 12 / 31
Amélioration des performances de surface des revêtements modernes grâce à la cire de polyéthylène oxydée
2025 / 12 / 30
Choisir le bon partenaire pour la cire de polyéthylène oxydé pour le CPVC - Ce qui compte vraiment et comment Rallychem le fait
2025 / 12 / 15

Pour toute demande de renseignements, veuillez appeler
Rallychem se fera un plaisir de vous aider !

+86 13456396233