Mengapa PVC menguning? Anda mungkin tidak pernah memahami 3 situasi ini secara sistematis
Anyone working with PVC knows that yellowing is a major problem that cannot be avoided.
Yellowing of pipes, dirtiness of sheets, graying of cables…not only affects appearance but can also impair performance.
But do you know why PVC yellows? And how can it be effectively prevented?
Today, we’ll provide a comprehensive analysis of the yellowing mechanism, prevention and control measures, and testing methods.
▶ Root cause: High-temperature processing and repeated heating break C-Cl bonds, generating HCl and forming a conjugated polyene structure (a chain of conjugated double bonds).
▶ Color development mechanism: The more conjugated double bonds there are, the stronger the π electron’s light absorption ability, causing the color to deepen from light yellow to orange-yellow to brown-red.
▶ Detection method: UV-Vis absorption spectroscopy: Detect the absorption peak between 250-450nm. Colorimeter: The higher the yellowing index Δb*, the darker the color.

▶ Reaction mechanism:
▶ Accelerated photooxidation: Chain reaction of reactive oxygen species (·O, ROOH) in the high-energy UV-A/B bands of UV light
▶ Cause:
▶ Additional Note: Some low-molecular-weight HALS are also susceptible to decomposition, especially in the presence of acidic substances (such as stearic acid), causing them to discolor more easily.
| Yellowing Types | Key Prevention Measures |
|---|---|
| Conjugated Double Bond Yellowing | Heat Stabilizer + Epoxy Compound + Temperature Control≤180°C |
| Oxidative Yellowing | Primary/Secondary Antioxidants + UV Absorbers + Titanium Dioxide/Coating Shielding |
| Yellowing Caused by Nitrogen-Containing Additives | Using Polymer HALS + Nitrogen-Free Alternatives + Metal Passivators |
PVC yellowing is a “chemical storm” caused by the combined effects of heat, light, and oxygen. To truly control it, we can’t rely solely on a single additive. Instead, we must develop a multi-faceted closed-loop approach encompassing formulation design, additive selection, processing control, and testing mechanisms. Only in this way can we achieve long-term anti-yellowing and stable appearance quality.
Anda Mungkin Tertarik
What Is PVC Lubricant and Why Is It Essential in PVC Processing?
2025 / 12 / 31
Enhancing Surface Performance in Modern Coatings with Oxidized Polyethylene Wax
2025 / 12 / 30
Memilih Mitra Lilin Polietilena Teroksidasi yang Tepat untuk CPVC - Apa yang Benar-Benar Penting dan Bagaimana Rallychem Memberikannya
2025 / 12 / 15
Mengoptimalkan Ekstrusi PVC dengan Lilin PE Teroksidasi - Bagaimana Aditif Kecil Memberikan Keuntungan Besar dalam Stabilitas Meleleh dan Kebersihan Die
2025 / 12 / 15
Rallychem Dipamerkan di Plast Eurasia Istanbul ke-34, Menciptakan Masa Depan yang Lebih Hijau Bersama Dunia
2025 / 12 / 08

Untuk pertanyaan, silakan hubungi
Rallychem Akan Dengan Senang Hati Membantu Anda!

+86 13456396233