Why is it so difficult to reach 60% chlorine content in CPVC pipe and dry mix?
Why did the national standard lower the chlorine content of CPVC pipe and dry mix from 60% to 55%?
Why is it so difficult to reach 60% chlorine content in CPVC?

Selection of high-quality raw materials: liquid-phase CPVC resin chlorine content is usually between 64% and 67%, which is more common. Solid-phase CPVC resin chlorine content can be more than 68%, but the color control is more difficult.
Application of efficient additives: Choose additives with small amount and high efficiency to reduce the dilution of chlorine content.
Innovative formulation ideas: Abandon the traditional PVC formulation mode, reduce the use of non-essential ingredients under the premise of ensuring processing convenience, so as to improve the overall chlorine content level.

Rallychem Chemical’s polyester wax and polyester homopolymer formulations are highly effective additives for CPVC production, providing excellent performance at lower usage levels, thereby reducing costs.
The use of polyester waxes and polyester homopolymers stabilizes the chlorine content of CPVC products at 58-59%, approaching 60%. In addition, we provide one-stop service to help customers reduce the need for production testing and adjustments, and provide them with efficient and economical production formulations and solutions.


Potreste essere interessati
What Is PVC Lubricant and Why Is It Essential in PVC Processing?
2025 / 12 / 31
Enhancing Surface Performance in Modern Coatings with Oxidized Polyethylene Wax
2025 / 12 / 30
Scegliere il giusto partner per la cera di polietilene ossidato per il CPVC: cosa conta davvero e come Rallychem lo offre
2025 / 12 / 15
Ottimizzazione dell'estrusione del PVC con la cera PE ossidata: come un piccolo additivo offre grandi vantaggi in termini di stabilità della colata e pulizia degli stampi
2025 / 12 / 15
Rallychem in mostra alla 34a edizione di Plast Eurasia Istanbul, per co-creare un futuro più verde con il mondo intero
2025 / 12 / 08