In the specification sheets for Oxidized Polyethylene (OPE) Wax, “density” is often just a number—typically ranging from 0.96 to 0.99 g/cm³. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential.
Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows technical teams to predict wear resistance, thermal stability, and emulsification behavior before a trial even begins.
Density reflects how closely polymer chains pack together:
Important: Density is not the same as oxidation level. The “oxidized” part relates to the introduction of polar groups (often reflected by parameters such as acid value), which can improve wetting/adhesion in certain systems.

In coatings and printing inks, hardness is directly linked to density. HDOPE waxes form substantially harder particles than LDOPE or standard paraffin. When these particles migrate to the surface (or are dispersed within the film), they act as “spacers” or slip agents that deflect physical stress.
HDOPE waxes typically soften and melt at higher temperatures (often >130°C, depending on grade) compared to low-density variants.
Because the polymer chains are linear and tightly packed, the wax itself is less brittle than low-molecular-weight by-products but harder than LDPE waxes.


Rallychem offers a comprehensive range of high-density oxidized polyethylene wax grades with carefully controlled density, melting points, molecular weights, and oxidation levels. These parameters can be adjusted to optimize wear resistance, hardness, thermal stability, slip, and scratch resistance across different application systems, including plastics, coatings, and printing inks.
By balancing polarity and molecular structure, our high-density oxidized polyethylene wax solutions ensure excellent dispersion and stable surface performance without compromising processing efficiency. Our technical experts work closely with customers to customize solutions that meet exact production conditions and performance requirements.

“High Density” in Oxidized Polyethylene Wax translates directly to physical durability and thermal resilience. By selecting a high-density grade, manufacturers can improve scratch resistance in coatings and stability in PVC extrusion, achieving high performance even at low dosages.
Rallychem offers a specialized series of HDOPE waxes with controlled density and oxidation levels. Whether you need a high-acid number for emulsions or a high-hardness grade for coatings, we can help match the spec to your application.
Rallychem cordially invites you to visit us at CHINA INTERDYE 2026 and explore advanced wax solutions designed for modern manufacturing challenges.
Exhibition: CHINA INTERDYE 2026
Date: 15–17 April 2026
Booth No.: H2 C621
Location: Shanghai, China
Rallychem | High-Density Oxidized PE Wax for Durable Surface Performance
ご興味があるかもしれません
PEワックスと酸化PEワックスの比較:PVCパイプ加工における潤滑性能の比較
2026 / 04 / 06
なぜエンジニアリングプラスチックには「特殊ワックス」が必要なのか? ラリーケム合成ポリエステルワックスの技術紹介
2026 / 04 / 02
PVCパイプの潤滑と強化の手引き:効率的で安定した押出成形のために、コストと性能の完璧なバランスを取る
2026 / 03 / 19
2026年の市場動向:水性ワックスエマルジョンが主要産業に与える影響
2026 / 03 / 04
PVCパイプ&プロファイル加工:熱安定剤が不可欠な理由と安定剤パッケージ内のワックス添加剤が重要な理由
2026 / 02 / 24