Lubricants in PVC Processing: A Comparison of OPE Wax and PE Wax
In the production of PVC products, selecting the appropriate lubricant is of paramount importance. Research from the University of South Africa, utilizing Scanning Electron Microscopy, has shed light on the differences in the micro-level effects of two common lubricants: Oxidized Polyethylene wax and Polyethylene wax.
Firstly, let’s explore the function of PE wax. As a non-polar substance, it is primarily used as an external lubricant because of its non-polarity, which allows it to operate effectively between PVC particles. It delays the plasticization process, preventing the resin from adhering to processing equipment. This characteristic is crucial for maintaining the smoothness of the processing operation, similar to the performance of Fischer-Tropsch wax.
Conversely, the polar nature of OPE wax enables it to bond with PVC resin, forming a uniform lubricating film that serves as an internal lubricant. Even under the shear applied during processing, it maintains stability and contributes to improved plasticization efficiency, which significantly enhances overall production efficiency. In the production of highly filled PVC products, the incorporation of OPE wax can effectively extend the service life of the screw, reducing maintenance costs.
It ensures smooth product demolding in the final stages of processing, which significantly reduces the waste rate. This is crucial for improving production efficiency and reducing costs.
In practical applications, the strategic selection of the appropriate type of wax, aligned with the specific requirements and production conditions of PVC products, can facilitate the optimization of formulations. This refined approach ensures a more efficient and cost-effective manufacturing process.
You May Be Interested
RALLYCHEM Shines at K 2025 Düsseldorf | Thank You for Joining Us!
2025 / 10 / 17
October in Düsseldorf — See You at K 2025
2025 / 09 / 30
랠리켐, 중국 플라스틱 파이프 협회 연례 회의 및 산업 교류 컨퍼런스 참석
2025 / 08 / 29
Frequent board breakage? Tame your extruder in three steps to eliminate PVC foam board brittleness.
2025 / 08 / 22
탄소 결정판 내부 윤활을 위한 새로운 옵션 | 안정적인 가격과 고효율의 전문 솔루션, 폴리에스테르 왁스 RL-1116F
2025 / 08 / 15