{"id":1732,"date":"2026-02-17T01:23:53","date_gmt":"2026-02-17T01:23:53","guid":{"rendered":"https:\/\/www.rallychem.com\/?p=1732"},"modified":"2026-02-24T02:06:29","modified_gmt":"2026-02-24T02:06:29","slug":"what-does-high-density-mean-in-oxidized-polyethylene-wax","status":"publish","type":"post","link":"https:\/\/www.rallychem.com\/ms\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","title":{"rendered":"Apakah maksud \u201cketumpatan tinggi\u201d dalam lilin polietilena teroksida?"},"content":{"rendered":"<p>Dalam helaian spesifikasi Lilin Polietilena Oksida (OPE), \u201cketumpatan\u201d sering kali hanya sekadar satu nombor\u2014biasanya antara 0.96 hingga 0.99 g\/cm\u00b3. Namun, bagi pembentuk formula dalam salutan, dakwat, dan pemprosesan PVC, nombor ini menceritakan kisah penting tentang struktur molekul dan potensi prestasi.<\/p>\n<p>Memahami perbezaan antara lilin Kepadatan Tinggi (HDOPE) dan Kepadatan Rendah (LDOPE) membolehkan pasukan teknikal meramalkan ketahanan haus, kestabilan termal, dan tingkah laku emulsi sebelum ujian dimulakan.<\/p>\n<p>&nbsp;<\/p>\n<h2><strong>Apakah maksud \u201cketumpatan tinggi\u201d sebenarnya?<\/strong><\/h2>\n<p>Kepadatan mencerminkan betapa rapat rantai polimer tersusun:<\/p>\n<ul>\n<li><b><\/b><strong><b>Struktur PE berketumpatan rendah: <\/b><\/strong>lebih banyak percabangan rantaian \u2192 ketebalan kristal lebih rendah \u2192 rasa lebih lembut<\/li>\n<li><b><\/b><strong><b>Struktur PE berketumpatan tinggi: <\/b><\/strong>rantaian linear yang lebih banyak \u2192 kekristalinan yang lebih tinggi \u2192 kekerasan yang lebih tinggi<\/li>\n<\/ul>\n<p>Penting: Kepekatan tidak sama dengan tahap pengoksidaan. Bahagian \u201cteroksida\u201d berkaitan dengan pengenalan kumpulan kutub (selalunya tercermin melalui parameter seperti nilai asid), yang boleh meningkatkan pembasahan\/pelekatan dalam sesetengah sistem.<\/p>\n<p><img decoding=\"async\" class=\"alignnone wp-image-1738\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-300x162.png\" alt=\"\" width=\"654\" height=\"353\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-300x162.png 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-768x415.png 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-18x10.png 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1.png 904w\" sizes=\"(max-width: 654px) 100vw, 654px\" \/><\/p>\n<p>&nbsp;<\/p>\n<h2><strong>Kelebihan Prestasi Utama Kepadatan Tinggi<\/strong><\/h2>\n<h3><strong><b>1. Ketahanan haus dan calar yang unggul<\/b><\/strong><\/h3>\n<p>Dalam salutan dan dakwat cetakan, kekerasan berkait rapat dengan ketumpatan. Lilin HDOPE membentuk zarah yang jauh lebih keras berbanding LDOPE atau parafin standard. Apabila zarah-zarah ini berhijrah ke permukaan (atau tersebar dalam filem), ia bertindak sebagai \u201cpenjarak\u201d atau ejen pelincir yang menangkis tegasan fizikal.<\/p>\n<ul>\n<li><b><\/b><strong><b>Keputusan: <\/b><\/strong>Ketahanan calar yang lebih baik pada salutan kayu, salutan gegelung, dan kemasan lantai.<\/li>\n<\/ul>\n<h3><strong><b>2. Keteguhan Terma yang Lebih Tinggi (Suhu Pencairan)<\/b><\/strong><\/h3>\n<p>Lilin HDOPE biasanya melembut dan mencair pada suhu yang lebih tinggi (selalunya &gt;130\u00b0C, bergantung pada gred) berbanding varian berketumpatan rendah.<\/p>\n<ul>\n<li><b><\/b><strong><b>Manfaat: <\/b><\/strong>Dalam pemprosesan plastik (seperti ekstrusi PVC keras), lilin kekal pepejal\/viskos lebih lama dalam laras ekstruder, menyediakan pelinciran luaran \u201ctertunda\u201d atau pelepasan logam di zon-zon kemudian tanpa terurai terlalu awal.<\/li>\n<\/ul>\n<h3><strong><b>3. Kekuatan Mekanikal yang Ditingkatkan<\/b><\/strong><\/h3>\n<p>Kerana rantaian polimer adalah lurus dan padat, lilin itu sendiri kurang rapuh berbanding hasil sampingan bermolekul berat rendah tetapi lebih keras daripada lilin LDPE.<\/p>\n<ul>\n<li><b><\/b><strong><b>Impak: <\/b><\/strong>Dalam pelekat lebur panas (HMA) atau komposit plastik, ia mengubah kelikatan tanpa mengorbankan integriti struktur atau titik pelembutan produk akhir seperti yang mungkin berlaku dengan lilin yang lebih lembut.<\/li>\n<\/ul>\n<p><img decoding=\"async\" class=\"wp-image-1733 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-300x200.jpeg\" alt=\"\" width=\"559\" height=\"372\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-300x200.jpeg 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-1024x683.jpeg 1024w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-768x512.jpeg 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-18x12.jpeg 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg 1269w\" sizes=\"(max-width: 559px) 100vw, 559px\" \/><\/p>\n<h2><strong>Aplikasi Tipikal<\/strong><\/h2>\n<p><img decoding=\"async\" class=\"wp-image-1740 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-300x252.png\" alt=\"\" width=\"585\" height=\"491\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-300x252.png 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-768x645.png 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-14x12.png 14w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2.png 863w\" sizes=\"(max-width: 585px) 100vw, 585px\" \/><\/p>\n<p>&nbsp;<\/p>\n<h2><strong>Memilih Lilin Polietilena Oksida Berketumpatan Tinggi yang Betul<\/strong><\/h2>\n<p>Rallychem menawarkan rangkaian komprehensif ketumpatan tinggi <span style=\"color: #cc99ff;\"><a style=\"color: #cc99ff;\" href=\"https:\/\/www.rallychem.com\/ms\/products\/oxidized-polyethylene-wax\/\"><u><span style=\"color: #ff00ff;\">Gred lilin polietilena teroksida<\/span><\/u><\/a><\/span>\u00a0dengan ketumpatan, titik lebur, berat molekul, dan tahap pengoksidaan yang dikawal dengan teliti. Parameter-parameter ini boleh disesuaikan untuk mengoptimumkan ketahanan haus, kekerasan, kestabilan terma, kelicinan, dan ketahanan calar dalam pelbagai sistem aplikasi, termasuk plastik, salutan, dan dakwat cetakan.<\/p>\n<p>Dengan mengimbangkan kutub dan struktur molekul, larutan lilin polietilena beroksida berketumpatan tinggi kami memastikan penyebaran yang cemerlang dan prestasi permukaan yang stabil tanpa menjejaskan kecekapan pemprosesan. Pakar teknikal kami bekerjasama rapat dengan pelanggan untuk menyesuaikan larutan yang memenuhi keadaan pengeluaran dan keperluan prestasi yang tepat.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-1734 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-300x216.jpeg\" alt=\"\" width=\"512\" height=\"368\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-300x216.jpeg 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-1024x737.jpeg 1024w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-768x553.jpeg 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-18x12.jpeg 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111.jpeg 1032w\" sizes=\"(max-width: 512px) 100vw, 512px\" \/><\/p>\n<h2><strong>Kesimpulan<\/strong><\/h2>\n<p>\u201cKetumpatan Tinggi\u201d dalam Lilin Polietilena Oksida secara langsung bermaksud ketahanan fizikal dan keteguhan termal. Dengan memilih gred ketumpatan tinggi, pengeluar boleh meningkatkan ketahanan calar pada salutan dan kestabilan dalam ekstrusi PVC, mencapai prestasi tinggi walaupun pada dos rendah.<\/p>\n<p>Rallychem menawarkan siri lilin HDOPE khusus dengan ketumpatan dan tahap pengoksidaan terkawal. Sama ada anda memerlukan nombor asid tinggi untuk emulsi atau gred kekerasan tinggi untuk salutan, kami boleh membantu menyesuaikan spesifikasi mengikut aplikasi anda.<\/p>\n<p>&nbsp;<\/p>\n<h2><strong>[Notis Acara] Temui Kami di CHINA INTERDYE 2026<\/strong><\/h2>\n<p>Rallychem dengan sukacitanya menjemput anda untuk melawat kami di CHINA INTERDYE 2026 dan meneroka penyelesaian lilin canggih yang direka untuk cabaran pembuatan moden.<\/p>\n<p><strong><b>Pameran<\/b><\/strong>: CHINA INTERDYE 2026<\/p>\n<p><strong><b>Tarikh<\/b><\/strong>: 15\u201317 April 2026<\/p>\n<p><strong><b>Gerai No.<\/b><\/strong>: H2 C621<\/p>\n<p><strong><b>Lokasi<\/b><\/strong>: Shanghai, China<\/p>\n<p>&nbsp;<\/p>\n<p><em>Rallychem | Lilin PE Teroksida Berketumpatan Tinggi untuk Prestasi Permukaan Tahan Lama<\/em><\/p>","protected":false},"excerpt":{"rendered":"<p>In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]<\/p>","protected":false},"author":4,"featured_media":1733,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[27,25],"tags":[57],"class_list":["post-1732","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-industry-news","category-news","tag-oxidized-polyethylene-wax"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v27.2 (Yoast SEO v27.2) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem<\/title>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/www.rallychem.com\/ms\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\" \/>\n<meta property=\"og:locale\" content=\"ms_MY\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\" \/>\n<meta property=\"og:description\" content=\"In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]\" \/>\n<meta property=\"og:url\" content=\"https:\/\/www.rallychem.com\/ms\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\" \/>\n<meta property=\"og:site_name\" content=\"Rallychem\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&amp;eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&amp;_rdr\" \/>\n<meta property=\"article:published_time\" content=\"2026-02-17T01:23:53+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2026-02-24T02:06:29+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\" \/>\n\t<meta property=\"og:image:width\" content=\"1269\" \/>\n\t<meta property=\"og:image:height\" content=\"846\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/jpeg\" \/>\n<meta name=\"author\" content=\"Qian\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:creator\" content=\"@Rallychem_\" \/>\n<meta name=\"twitter:site\" content=\"@Rallychem_\" \/>\n<meta name=\"twitter:label1\" content=\"Written by\" \/>\n\t<meta name=\"twitter:data1\" content=\"Qian\" \/>\n\t<meta name=\"twitter:label2\" content=\"Est. reading time\" \/>\n\t<meta name=\"twitter:data2\" content=\"3 minit\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#article\",\"isPartOf\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"},\"author\":{\"name\":\"Qian\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604\"},\"headline\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\",\"datePublished\":\"2026-02-17T01:23:53+00:00\",\"dateModified\":\"2026-02-24T02:06:29+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"},\"wordCount\":557,\"publisher\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"keywords\":[\"Oxidized polyethylene wax\"],\"articleSection\":[\"Industry News\",\"News\"],\"inLanguage\":\"ms-MY\"},{\"@type\":\"WebPage\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\",\"url\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\",\"name\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem\",\"isPartOf\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"datePublished\":\"2026-02-17T01:23:53+00:00\",\"dateModified\":\"2026-02-24T02:06:29+00:00\",\"breadcrumb\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb\"},\"inLanguage\":\"ms-MY\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"ms-MY\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\",\"url\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"contentUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"width\":1269,\"height\":846},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\/\/www.rallychem.com\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#website\",\"url\":\"https:\/\/www.rallychem.com\/de\/\",\"name\":\"Rallychem\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/www.rallychem.com\/de\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ms-MY\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\",\"name\":\"Rallychem\",\"url\":\"https:\/\/www.rallychem.com\/de\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ms-MY\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/\",\"url\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg\",\"contentUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg\",\"width\":566,\"height\":566,\"caption\":\"Rallychem\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/\"},\"sameAs\":[\"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr\",\"https:\/\/x.com\/Rallychem_\",\"https:\/\/www.linkedin.com\/company\/rallychem\/posts\/?feedView=all\",\"https:\/\/www.youtube.com\/@Rallychem\"]},{\"@type\":\"Person\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604\",\"name\":\"Qian\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ms-MY\",\"@id\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"url\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"contentUrl\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"caption\":\"Qian\"},\"url\":\"https:\/\/www.rallychem.com\/ms\/author\/qian\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"Apakah maksud \u201cketumpatan tinggi\u201d dalam lilin polietilena teroksida? - Rallychem","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/www.rallychem.com\/ms\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","og_locale":"ms_MY","og_type":"article","og_title":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?","og_description":"In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]","og_url":"https:\/\/www.rallychem.com\/ms\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","og_site_name":"Rallychem","article_publisher":"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr","article_published_time":"2026-02-17T01:23:53+00:00","article_modified_time":"2026-02-24T02:06:29+00:00","og_image":[{"width":1269,"height":846,"url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","type":"image\/jpeg"}],"author":"Qian","twitter_card":"summary_large_image","twitter_creator":"@Rallychem_","twitter_site":"@Rallychem_","twitter_misc":{"Written by":"Qian","Est. reading time":"3 minit"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#article","isPartOf":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"},"author":{"name":"Qian","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604"},"headline":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?","datePublished":"2026-02-17T01:23:53+00:00","dateModified":"2026-02-24T02:06:29+00:00","mainEntityOfPage":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"},"wordCount":557,"publisher":{"@id":"https:\/\/www.rallychem.com\/de\/#organization"},"image":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"thumbnailUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","keywords":["Oxidized polyethylene wax"],"articleSection":["Industry News","News"],"inLanguage":"ms-MY"},{"@type":"WebPage","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","url":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","name":"Apakah maksud \u201cketumpatan tinggi\u201d dalam lilin polietilena teroksida? - Rallychem","isPartOf":{"@id":"https:\/\/www.rallychem.com\/de\/#website"},"primaryImageOfPage":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"image":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"thumbnailUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","datePublished":"2026-02-17T01:23:53+00:00","dateModified":"2026-02-24T02:06:29+00:00","breadcrumb":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb"},"inLanguage":"ms-MY","potentialAction":[{"@type":"ReadAction","target":["https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"]}]},{"@type":"ImageObject","inLanguage":"ms-MY","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage","url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","contentUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","width":1269,"height":846},{"@type":"BreadcrumbList","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/www.rallychem.com\/"},{"@type":"ListItem","position":2,"name":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?"}]},{"@type":"WebSite","@id":"https:\/\/www.rallychem.com\/de\/#website","url":"https:\/\/www.rallychem.com\/de\/","name":"Rallychem","description":"","publisher":{"@id":"https:\/\/www.rallychem.com\/de\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/www.rallychem.com\/de\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ms-MY"},{"@type":"Organization","@id":"https:\/\/www.rallychem.com\/de\/#organization","name":"Rallychem","url":"https:\/\/www.rallychem.com\/de\/","logo":{"@type":"ImageObject","inLanguage":"ms-MY","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/","url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg","contentUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg","width":566,"height":566,"caption":"Rallychem"},"image":{"@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr","https:\/\/x.com\/Rallychem_","https:\/\/www.linkedin.com\/company\/rallychem\/posts\/?feedView=all","https:\/\/www.youtube.com\/@Rallychem"]},{"@type":"Person","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604","name":"Qian","image":{"@type":"ImageObject","inLanguage":"ms-MY","@id":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","caption":"Qian"},"url":"https:\/\/www.rallychem.com\/ms\/author\/qian\/"}]}},"_links":{"self":[{"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/posts\/1732","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/users\/4"}],"replies":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/comments?post=1732"}],"version-history":[{"count":7,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/posts\/1732\/revisions"}],"predecessor-version":[{"id":1744,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/posts\/1732\/revisions\/1744"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/media\/1733"}],"wp:attachment":[{"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/media?parent=1732"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/categories?post=1732"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.rallychem.com\/ms\/wp-json\/wp\/v2\/tags?post=1732"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}