{"id":1732,"date":"2026-02-17T01:23:53","date_gmt":"2026-02-17T01:23:53","guid":{"rendered":"https:\/\/www.rallychem.com\/?p=1732"},"modified":"2026-02-24T02:06:29","modified_gmt":"2026-02-24T02:06:29","slug":"what-does-high-density-mean-in-oxidized-polyethylene-wax","status":"publish","type":"post","link":"https:\/\/www.rallychem.com\/th\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","title":{"rendered":"\u201c\u0e04\u0e27\u0e32\u0e21\u0e2b\u0e19\u0e32\u0e41\u0e19\u0e48\u0e19\u0e2a\u0e39\u0e07\u201d \u0e2b\u0e21\u0e32\u0e22\u0e16\u0e36\u0e07\u0e2d\u0e30\u0e44\u0e23\u0e43\u0e19\u0e41\u0e27\u0e47\u0e01\u0e0b\u0e4c\u0e42\u0e1e\u0e25\u0e35\u0e40\u0e2d\u0e17\u0e34\u0e25\u0e35\u0e19\u0e2d\u0e2d\u0e01\u0e44\u0e0b\u0e14\u0e4c?"},"content":{"rendered":"<p>In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential.<\/p>\n<p>Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows technical teams to predict wear resistance, thermal stability, and emulsification behavior before a trial even begins.<\/p>\n<p>&nbsp;<\/p>\n<h2><strong>What Does \u201cHigh Density\u201d Actually Mean?<\/strong><\/h2>\n<p>Density\u00a0reflects how closely polymer chains pack together:<\/p>\n<ul>\n<li><b><\/b><strong><b>Lower-density PE structures: <\/b><\/strong>more chain branching \u2192 lower crystallinity \u2192 softer feel<\/li>\n<li><b><\/b><strong><b>Higher-density PE structures: <\/b><\/strong>more linear chains \u2192 higher crystallinity \u2192 higher hardness<\/li>\n<\/ul>\n<p>Important:\u00a0Density is\u00a0not the same as oxidation level. The \u201coxidized\u201d part relates to the\u00a0introduction of polar groups\u00a0(often reflected by parameters such as acid value), which can improve wetting\/adhesion in certain systems.<\/p>\n<p><img decoding=\"async\" class=\"alignnone wp-image-1738\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-300x162.png\" alt=\"\" width=\"654\" height=\"353\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-300x162.png 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-768x415.png 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1-18x10.png 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/1.png 904w\" sizes=\"(max-width: 654px) 100vw, 654px\" \/><\/p>\n<p>&nbsp;<\/p>\n<h2><strong>Key Performance Advantages of High Density<\/strong><\/h2>\n<h3><strong><b>1. Superior Wear and Scratch Resistance<\/b><\/strong><\/h3>\n<p>In coatings and printing inks, hardness is directly linked to density. HDOPE waxes form substantially harder particles than LDOPE or standard paraffin. When these particles migrate to the surface (or are dispersed within the film), they act as &#8220;spacers&#8221; or slip agents that deflect physical stress.<\/p>\n<ul>\n<li><b><\/b><strong><b>Result: <\/b><\/strong>Better scratch resistance in wood coatings, coil coatings, and floor finishes.<\/li>\n<\/ul>\n<h3><strong><b>2. Higher Thermal Stability (Melting Point)<\/b><\/strong><\/h3>\n<p>HDOPE waxes typically soften and melt at higher temperatures (often &gt;130\u00b0C, depending on grade) compared to low-density variants.<\/p>\n<ul>\n<li><b><\/b><strong><b>Benefit: <\/b><\/strong>In plastics processing (like rigid PVC extrusion), the wax remains solid\/viscous longer in the extruder barrel, providing &#8220;delayed&#8221; external lubrication or metal release in later zones without degrading too early.<\/li>\n<\/ul>\n<h3><strong><b>3. Improved Mechanical Strength<\/b><\/strong><\/h3>\n<p>Because the polymer chains are linear and tightly packed, the wax itself is less brittle than low-molecular-weight by-products but harder than LDPE waxes.<\/p>\n<ul>\n<li><b><\/b><strong><b>Impact: <\/b><\/strong>In hot melt adhesives (HMA) or plastic composites, it modifies viscosity without sacrificing the structural integrity or softening point of the final product as much as softer waxes might.<\/li>\n<\/ul>\n<p><img decoding=\"async\" class=\"wp-image-1733 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-300x200.jpeg\" alt=\"\" width=\"559\" height=\"372\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-300x200.jpeg 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-1024x683.jpeg 1024w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-768x512.jpeg 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111-18x12.jpeg 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg 1269w\" sizes=\"(max-width: 559px) 100vw, 559px\" \/><\/p>\n<h2><strong>Typical Applications<\/strong><\/h2>\n<p><img decoding=\"async\" class=\"wp-image-1740 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-300x252.png\" alt=\"\" width=\"585\" height=\"491\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-300x252.png 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-768x645.png 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2-14x12.png 14w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/2.png 863w\" sizes=\"(max-width: 585px) 100vw, 585px\" \/><\/p>\n<p>&nbsp;<\/p>\n<h2><strong>Choosing the Right High-Density Oxidized Polyethylene Wax<\/strong><\/h2>\n<p>Rallychem offers a comprehensive range of high-density <span style=\"color: #cc99ff;\"><a style=\"color: #cc99ff;\" href=\"https:\/\/www.rallychem.com\/th\/products\/oxidized-polyethylene-wax\/\"><u><span style=\"color: #ff00ff;\">oxidized polyethylene wax grades<\/span><\/u><\/a><\/span>\u00a0with carefully controlled density, melting points, molecular weights, and oxidation levels. These parameters can be adjusted to optimize wear resistance, hardness, thermal stability, slip, and scratch resistance across different application systems, including plastics, coatings, and printing inks.<\/p>\n<p>By balancing polarity and molecular structure, our high-density oxidized polyethylene wax solutions ensure excellent dispersion and stable surface performance without compromising processing efficiency. Our technical experts work closely with customers to customize solutions that meet exact production conditions and performance requirements.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-1734 aligncenter\" src=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-300x216.jpeg\" alt=\"\" width=\"512\" height=\"368\" srcset=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-300x216.jpeg 300w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-1024x737.jpeg 1024w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-768x553.jpeg 768w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111-18x12.jpeg 18w, https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/WPS\u56fe\u724711111.jpeg 1032w\" sizes=\"(max-width: 512px) 100vw, 512px\" \/><\/p>\n<h2><strong>\u0e2a\u0e23\u0e38\u0e1b<\/strong><\/h2>\n<p>&#8220;High Density&#8221; in Oxidized Polyethylene Wax translates directly to physical durability and thermal resilience. By selecting a high-density grade, manufacturers can improve scratch resistance in coatings and stability in PVC extrusion, achieving high performance even at low dosages.<\/p>\n<p>Rallychem offers a specialized series of HDOPE waxes with controlled density and oxidation levels. Whether you need a high-acid number for emulsions or a high-hardness grade for coatings, we can help match the spec to your application.<\/p>\n<p>&nbsp;<\/p>\n<h2><strong>[Event Notice] Meet Us at CHINA INTERDYE 2026<\/strong><\/h2>\n<p>Rallychem cordially invites you to visit us at CHINA INTERDYE 2026 and explore advanced wax solutions designed for modern manufacturing challenges.<\/p>\n<p><strong><b>Exhibition<\/b><\/strong>: CHINA INTERDYE 2026<\/p>\n<p><strong><b>Date<\/b><\/strong>: 15\u201317 April 2026<\/p>\n<p><strong><b>Booth No.<\/b><\/strong>: H2 C621<\/p>\n<p><strong><b>Location<\/b><\/strong>: Shanghai, China<\/p>\n<p>&nbsp;<\/p>\n<p><em>Rallychem | High-Density Oxidized PE Wax for Durable Surface Performance<\/em><\/p>","protected":false},"excerpt":{"rendered":"<p>In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]<\/p>","protected":false},"author":4,"featured_media":1733,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[27,25],"tags":[57],"class_list":["post-1732","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-industry-news","category-news","tag-oxidized-polyethylene-wax"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v27.2 (Yoast SEO v27.2) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem<\/title>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/www.rallychem.com\/th\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\" \/>\n<meta property=\"og:locale\" content=\"th_TH\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\" \/>\n<meta property=\"og:description\" content=\"In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]\" \/>\n<meta property=\"og:url\" content=\"https:\/\/www.rallychem.com\/th\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\" \/>\n<meta property=\"og:site_name\" content=\"Rallychem\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&amp;eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&amp;_rdr\" \/>\n<meta property=\"article:published_time\" content=\"2026-02-17T01:23:53+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2026-02-24T02:06:29+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\" \/>\n\t<meta property=\"og:image:width\" content=\"1269\" \/>\n\t<meta property=\"og:image:height\" content=\"846\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/jpeg\" \/>\n<meta name=\"author\" content=\"Qian\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:creator\" content=\"@Rallychem_\" \/>\n<meta name=\"twitter:site\" content=\"@Rallychem_\" \/>\n<meta name=\"twitter:label1\" content=\"Written by\" \/>\n\t<meta name=\"twitter:data1\" content=\"Qian\" \/>\n\t<meta name=\"twitter:label2\" content=\"Est. reading time\" \/>\n\t<meta name=\"twitter:data2\" content=\"3 \u0e19\u0e32\u0e17\u0e35\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#article\",\"isPartOf\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"},\"author\":{\"name\":\"Qian\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604\"},\"headline\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\",\"datePublished\":\"2026-02-17T01:23:53+00:00\",\"dateModified\":\"2026-02-24T02:06:29+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"},\"wordCount\":557,\"publisher\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"keywords\":[\"Oxidized polyethylene wax\"],\"articleSection\":[\"Industry News\",\"News\"],\"inLanguage\":\"th\"},{\"@type\":\"WebPage\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\",\"url\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\",\"name\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem\",\"isPartOf\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"datePublished\":\"2026-02-17T01:23:53+00:00\",\"dateModified\":\"2026-02-24T02:06:29+00:00\",\"breadcrumb\":{\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb\"},\"inLanguage\":\"th\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"th\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage\",\"url\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"contentUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg\",\"width\":1269,\"height\":846},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\/\/www.rallychem.com\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#website\",\"url\":\"https:\/\/www.rallychem.com\/de\/\",\"name\":\"Rallychem\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/www.rallychem.com\/de\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"th\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#organization\",\"name\":\"Rallychem\",\"url\":\"https:\/\/www.rallychem.com\/de\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"th\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/\",\"url\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg\",\"contentUrl\":\"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg\",\"width\":566,\"height\":566,\"caption\":\"Rallychem\"},\"image\":{\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/\"},\"sameAs\":[\"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr\",\"https:\/\/x.com\/Rallychem_\",\"https:\/\/www.linkedin.com\/company\/rallychem\/posts\/?feedView=all\",\"https:\/\/www.youtube.com\/@Rallychem\"]},{\"@type\":\"Person\",\"@id\":\"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604\",\"name\":\"Qian\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"th\",\"@id\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"url\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"contentUrl\":\"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g\",\"caption\":\"Qian\"},\"url\":\"https:\/\/www.rallychem.com\/th\/author\/qian\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/www.rallychem.com\/th\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","og_locale":"th_TH","og_type":"article","og_title":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?","og_description":"In the specification sheets for Oxidized Polyethylene (OPE) Wax, &#8220;density&#8221; is often just a number\u2014typically ranging from 0.96 to 0.99 g\/cm\u00b3. However, for formulators in coatings, inks, and PVC processing, this number tells a crucial story about molecular structure and performance potential. Understanding the difference between High Density (HDOPE) and Low Density (LDOPE) waxes allows [&hellip;]","og_url":"https:\/\/www.rallychem.com\/th\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","og_site_name":"Rallychem","article_publisher":"https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr","article_published_time":"2026-02-17T01:23:53+00:00","article_modified_time":"2026-02-24T02:06:29+00:00","og_image":[{"width":1269,"height":846,"url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","type":"image\/jpeg"}],"author":"Qian","twitter_card":"summary_large_image","twitter_creator":"@Rallychem_","twitter_site":"@Rallychem_","twitter_misc":{"Written by":"Qian","Est. reading time":"3 \u0e19\u0e32\u0e17\u0e35"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#article","isPartOf":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"},"author":{"name":"Qian","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604"},"headline":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?","datePublished":"2026-02-17T01:23:53+00:00","dateModified":"2026-02-24T02:06:29+00:00","mainEntityOfPage":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"},"wordCount":557,"publisher":{"@id":"https:\/\/www.rallychem.com\/de\/#organization"},"image":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"thumbnailUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","keywords":["Oxidized polyethylene wax"],"articleSection":["Industry News","News"],"inLanguage":"th"},{"@type":"WebPage","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","url":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/","name":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax? - Rallychem","isPartOf":{"@id":"https:\/\/www.rallychem.com\/de\/#website"},"primaryImageOfPage":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"image":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage"},"thumbnailUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","datePublished":"2026-02-17T01:23:53+00:00","dateModified":"2026-02-24T02:06:29+00:00","breadcrumb":{"@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb"},"inLanguage":"th","potentialAction":[{"@type":"ReadAction","target":["https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/"]}]},{"@type":"ImageObject","inLanguage":"th","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#primaryimage","url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","contentUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/02\/111.jpeg","width":1269,"height":846},{"@type":"BreadcrumbList","@id":"https:\/\/www.rallychem.com\/news\/industry-news\/what-does-high-density-mean-in-oxidized-polyethylene-wax\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/www.rallychem.com\/"},{"@type":"ListItem","position":2,"name":"What Does \u201cHigh Density\u201d Mean in Oxidized Polyethylene Wax?"}]},{"@type":"WebSite","@id":"https:\/\/www.rallychem.com\/de\/#website","url":"https:\/\/www.rallychem.com\/de\/","name":"\u0e41\u0e23\u0e25\u0e25\u0e35\u0e48\u0e40\u0e04\u0e21","description":"","publisher":{"@id":"https:\/\/www.rallychem.com\/de\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/www.rallychem.com\/de\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"th"},{"@type":"Organization","@id":"https:\/\/www.rallychem.com\/de\/#organization","name":"\u0e41\u0e23\u0e25\u0e25\u0e35\u0e48\u0e40\u0e04\u0e21","url":"https:\/\/www.rallychem.com\/de\/","logo":{"@type":"ImageObject","inLanguage":"th","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/","url":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg","contentUrl":"https:\/\/www.rallychem.com\/wp-content\/uploads\/2026\/03\/rallychem-logo.jpg","width":566,"height":566,"caption":"Rallychem"},"image":{"@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/p\/Shanghai-Rallychem-Chemicals-Co-LTD-100069762685039\/?paipv=0&eav=AfZYRDGpo9gzk-dMgbaOJ2wHvxYFzzxSvLdcXizI3FOgfgyxNlKfr_tlTEWZSxgpDpo&_rdr","https:\/\/x.com\/Rallychem_","https:\/\/www.linkedin.com\/company\/rallychem\/posts\/?feedView=all","https:\/\/www.youtube.com\/@Rallychem"]},{"@type":"Person","@id":"https:\/\/www.rallychem.com\/de\/#\/schema\/person\/de35b8d71f6ee7ea28e1114b8798a604","name":"Qian","image":{"@type":"ImageObject","inLanguage":"th","@id":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/c5e43227d9ae338abe363967095fee86321ee647c7174ebd3381245990358a23?s=96&d=mm&r=g","caption":"Qian"},"url":"https:\/\/www.rallychem.com\/th\/author\/qian\/"}]}},"_links":{"self":[{"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/posts\/1732","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/users\/4"}],"replies":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/comments?post=1732"}],"version-history":[{"count":7,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/posts\/1732\/revisions"}],"predecessor-version":[{"id":1744,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/posts\/1732\/revisions\/1744"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/media\/1733"}],"wp:attachment":[{"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/media?parent=1732"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/categories?post=1732"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.rallychem.com\/th\/wp-json\/wp\/v2\/tags?post=1732"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}