PVC neden sararır? Bu 3 durumu sistematik olarak hiç anlamamış olabilirsiniz
Anyone working with PVC knows that yellowing is a major problem that cannot be avoided.
Yellowing of pipes, dirtiness of sheets, graying of cables…not only affects appearance but can also impair performance.
But do you know why PVC yellows? And how can it be effectively prevented?
Today, we’ll provide a comprehensive analysis of the yellowing mechanism, prevention and control measures, and testing methods.
▶ Root cause: High-temperature processing and repeated heating break C-Cl bonds, generating HCl and forming a conjugated polyene structure (a chain of conjugated double bonds).
▶ Color development mechanism: The more conjugated double bonds there are, the stronger the π electron’s light absorption ability, causing the color to deepen from light yellow to orange-yellow to brown-red.
▶ Detection method: UV-Vis absorption spectroscopy: Detect the absorption peak between 250-450nm. Colorimeter: The higher the yellowing index Δb*, the darker the color.
▶ Reaction mechanism:
▶ Accelerated photooxidation: Chain reaction of reactive oxygen species (·O, ROOH) in the high-energy UV-A/B bands of UV light
▶ Cause:
▶ Additional Note: Some low-molecular-weight HALS are also susceptible to decomposition, especially in the presence of acidic substances (such as stearic acid), causing them to discolor more easily.
| Yellowing Types | Key Prevention Measures |
|---|---|
| Conjugated Double Bond Yellowing | Heat Stabilizer + Epoxy Compound + Temperature Control≤180°C |
| Oxidative Yellowing | Primary/Secondary Antioxidants + UV Absorbers + Titanium Dioxide/Coating Shielding |
| Yellowing Caused by Nitrogen-Containing Additives | Using Polymer HALS + Nitrogen-Free Alternatives + Metal Passivators |
PVC yellowing is a “chemical storm” caused by the combined effects of heat, light, and oxygen. To truly control it, we can’t rely solely on a single additive. Instead, we must develop a multi-faceted closed-loop approach encompassing formulation design, additive selection, processing control, and testing mechanisms. Only in this way can we achieve long-term anti-yellowing and stable appearance quality.
İlginizi Çekebilir
Mühendislik Plastikleri Yağlaması: Polyester Wax Neden Montan Wax Alternatifidir?
2026 / 01 / 23
RallyChem'in Gelişmiş Wax Katkıları ile Kaplama Dayanıklılığını Optimize Etme
2026 / 01 / 22
PVC Yağlayıcı Nedir ve PVC İşlemede Neden Önemlidir?
2025 / 12 / 31
Okside Polietilen Balmumu ile Modern Kaplamalarda Yüzey Performansının Artırılması
2025 / 12 / 30
CPVC için Doğru Okside Polietilen Balmumu Ortağını Seçmek - Gerçekten Önemli Olan Nedir ve Rallychem Nasıl Sunar?
2025 / 12 / 15

Sorularınız İçin Lütfen Arayınız
Rallychem Size Yardımcı Olmaktan Mutluluk Duyacaktır!
+86 13456396233