2022 / 08 / 01
What does the acid value of oxidized polyethylene wax represent in PVC processing?

Oxidized polyethylene waxes are used as both internal and external PVC lubricants. There are a number of common models on the market, such as 916, 925 and 930, which represent acid value 16, acid value 25 and acid value 30, respectively.
Generally speaking, the acid value represents the polarity of the oxidized wax and is positively correlated. The higher the acid value, the higher the polarity of the oxidized wax. In practical PVC processing, a higher acid value means that the oxidized wax has a more pronounced internal lubrication effect and increases the speed of plasticization. For example, the plasticizing speed of 930 with acid value 30 is significantly faster than that of 916 with acid value 16, so it is more suitable for PVC products with higher plasticizing requirements, such as SPC flooring, stone wall panels and other highly filled products.

On the other hand, when the acid value of oxidized polyethylene wax is higher, it is more in favor of internal lubrication, and its external lubrication effect will be relatively weakened. Therefore, oxidized polyethylene waxes with low acid values are more suitable for PVC products with high demands on post-molding and surface. For example, shrink films, calendered sheets, etc.


Therefore, 916A with an acid value of 16 can be used as a good late release agent after plasticization has reached the required level.
İlginizi Çekebilir
RALLYCHEM K 2025 Düsseldorf'ta Parlıyor | Bize Katıldığınız İçin Teşekkür Ederiz!
2025 / 10 / 17
Düsseldorf'ta Ekim Ayı - K 2025'te Görüşmek Üzere
2025 / 09 / 30
Rallychem, Çin Plastik Boru Birliği Yıllık Toplantısı ve Endüstri Değişim Konferansına katıldı
2025 / 08 / 29
Sık sık levha kırılıyor mu? PVC köpük levha kırılganlığını ortadan kaldırmak için ekstrüderinizi üç adımda evcilleştirin.
2025 / 08 / 22
Karbon kristal plaka iç yağlaması için yeni bir seçenek | Polyester wax RL-1116F, istikrarlı fiyat ve yüksek verimlilik ile profesyonel bir çözüm
2025 / 08 / 15

Sorularınız İçin Lütfen Arayınız
Rallychem Size Yardımcı Olmaktan Mutluluk Duyacaktır!

+86 13456396233