    Balance of Toughness and Rigidity

    Enhance Physical Properties

    Avoid Issues from Over-Lubrication

  • Lợi thế về chi phí

    Extend Screw Life

  • Lợi thế sản xuất

    Enhance Plasticizing Speed and Production Efficiency

    Prolong Operating Time

    Improve Filler Dispersion

Câu hỏi thường gặp

  • High filler loading keeps biting you—what should you tweak first?

    +

    Start with how your additives work together. When CaCO3 is heavy, you want better dispersion and fewer friction hot spots. That means:

    · Use a polar polyester wax inside the melt (internal lube) to spread fillers evenly and cool down those hotspots.

    · Pair it with an external lube to keep surfaces smooth without over-slicking the melt.

    · Add a polyester homopolymer for toughness, without making the sheet “rubbery.”

    Goal: fewer white residues on rolls and screws, less charring, cleaner surfaces, and a faster line.

  • What’s special about polar polyester waxes here?

    +

    They’re the “good roommates” in PVC-more compatible, so they stay put. Result:

    · Better filler dispersion

    · Lower friction heat and fewer brown spots

    · Less oily surface and less migration

    Perfect for CaCO3-rich floor/wall lines that need both dispersion and screw life.

  • How do you balance lubrication without killing mechanics?

    +

    Split the jobs:

    · Internal: polar polyester wax (helps fusion and dispersion)

    · External: high-density oxidized PE wax (helps release and gloss)

    We found the sweet spot is the minimum effective dose. If you see mechanicals dip, bring in a polyester homopolymer to get toughness back.

Rallychem Chemicals sẽ cung cấp cho quý khách hàng các dịch vụ tư vấn chuyên nghiệp, giải pháp tùy chỉnh cho PVC/CPVC, phụ gia sáp, nhũ tương sáp, dịch vụ sản xuất tùy chỉnh các polymer vi mô. Mời quý khách hàng liên hệ với chúng tôi.

Liên hệ với chúng tôi

WhatsApp

Để biết thêm thông tin, vui lòng liên hệ qua số điện thoại.

Rallychem rất hân hạnh được hỗ trợ quý khách!

+86 13456396233