Q:What are the main index requirements of CPVC power pipe?
A: Vickers reaches above 93℃, and can pass the ring stiffness, flatness and drop hammer impact test. These rigid requirements ensure its insulation and corrosion resistance, which can better protect the cables.
Q: So what are the main index requirements for CPVC plumbing pipes?
A: CPVC hot and cold water pipes should be more heat and pressure resistant, with a Vickers greater than 110°C and a tensile yield stress of more than 50MPa to ensure it is safe and reliable.
Q:What are the main index requirements for CPVC industrial pipe?
A: In order to ensure that CPVC industrial pipe should be reliable even under extreme conditions, its Vicat should be greater than 110℃, tensile strength should be greater than 50MPa, and chlorine content should be more than 55%.
Q: Finally, what are some of the high standard characteristics of CPVC fire protection pipe?
A: As a life support in emergency situations, CPVC fire hose has the highest requirements. The Vickers has to reach 113°C and the chlorine content is also required to be over 60%.
Q: How do the four major CPVC pipes have to meet these high standards?
A: Rallychem Chemicals specializes in CPVC solutions, providing customers with turnkey services, helping customers produce stable and qualified CPVC products earlier, seizing the market opportunity, saving money, time and technology.
Bạn có thể quan tâm
New Product Teaser|Entering the Era of “Stability Competition” in Engineering Plastics, a True Montan Wax Replacement Solution Has Arrived
2026 / 04 / 20
Rallychem Advanced Materials ── From Material Behavior to Process-Controlled Performance
2026 / 04 / 16
Sáp PE so với sáp PE oxy hóa: So sánh hiệu suất bôi trơn trong quá trình gia công ống PVC
2026 / 04 / 06
Tại sao nhựa kỹ thuật lại cần một loại “sáp đặc biệt”? Giới thiệu kỹ thuật về sáp polyester tổng hợp Rallychem
2026 / 04 / 02
Hướng dẫn bôi trơn và tăng cường độ bền cho ống PVC: Tìm kiếm sự cân bằng hoàn hảo giữa chi phí và hiệu suất để đạt được quá trình đùn hiệu quả và ổn định
2026 / 03 / 19

Để biết thêm thông tin, vui lòng liên hệ qua số điện thoại.
Rallychem rất hân hạnh được hỗ trợ quý khách!

+86 13456396233