Nuestras ventajas

  • Ventaja de rendimiento

    Applicable to Transparent Products

    Tougher, Less Exudation

  • Ventaja de costes

    Reduces Mold Clearing Frequency, Lowering Costs

  • Ventaja de producción

    Prolongs Start-up Time

    Low Impact on Printing Performance

Preguntas frecuentes

  • Why do you get plate-out in high-speed calendering or blown film?

    +

    Same story: high shear and heat push low-compatibility, low-MW additives to migrate or volatilize. Use polar polyester waxes plus polyester homopolymers to improve compatibility and melt stability, so less buildup and longer time between die cleanups.

  • How do you toughen films/sheets without making them gummy?

    +

    Polyester homopolymers create tiny energy absorbers, lifting elongation and tensile strength, improving impact and crack resistance.

    · For clear grades, go low-color, low-VOC.

    · Pair with polar polyester wax for stable processing and a clean surface.

  • Will additives mess with printing?

    +

    Internal polar polyester waxes (low VOC, low migration) reduce surface oiliness and actually help ink adhesion compared to typical non-polar lubes. Still, do your surface treatment/cleaning and run an adhesion test.

Rallychem Chemicals le proporcionará servicios profesionales de consultoría, servicios de soluciones personalizadas de PVC/CPVC, aditivos de cera, emulsiones de cera, servicios de producción personalizada de micropolímeros, le invitamos a ponerse en contacto con nosotros.

Póngase en contacto con nosotros

WhatsApp

Para más información, llame al

Rallychem estará encantado de ayudarle.

+86 13456396233