Oxidized polyethylene waxes are used as both internal and external PVC lubricants. There are a number of common models on the market, such as 916, 925 and 930, which represent acid value 16, acid value 25 and acid value 30, respectively.
Generally speaking, the acid value represents the polarity of the oxidized wax and is positively correlated. The higher the acid value, the higher the polarity of the oxidized wax. In practical PVC processing, a higher acid value means that the oxidized wax has a more pronounced internal lubrication effect and increases the speed of plasticization. For example, the plasticizing speed of 930 with acid value 30 is significantly faster than that of 916 with acid value 16, so it is more suitable for PVC products with higher plasticizing requirements, such as SPC flooring, stone wall panels and other highly filled products.

On the other hand, when the acid value of oxidized polyethylene wax is higher, it is more in favor of internal lubrication, and its external lubrication effect will be relatively weakened. Therefore, oxidized polyethylene waxes with low acid values are more suitable for PVC products with high demands on post-molding and surface. For example, shrink films, calendered sheets, etc.


Therefore, 916A with an acid value of 16 can be used as a good late release agent after plasticization has reached the required level.
Quizá le interese
New Product Teaser|Entering the Era of “Stability Competition” in Engineering Plastics, a True Montan Wax Replacement Solution Has Arrived
2026 / 04 / 20
Rallychem Advanced Materials ── From Material Behavior to Process-Controlled Performance
2026 / 04 / 16
Cera de PE frente a cera de PE oxidada: Comparación del rendimiento de la lubricación en el procesamiento de tuberías de PVC
2026 / 04 / 06
¿Por qué los plásticos técnicos necesitan una “cera especial”? Introducción técnica a la cera sintética de poliéster Rallychem
2026 / 04 / 02
Guía de lubricación y endurecimiento de tuberías de PVC: El equilibrio perfecto entre coste y rendimiento para una extrusión estable y eficaz
2026 / 03 / 19