RL-501

Inquire
  • Product Information

  • Technical Data

  • Wax Type

    Liquid EP plasticizer

  • Model

    RL-501

  • Industry & Functionality

    PVC products

    reduces the probability of scorching during the production and helps to improve the yield.

  • Specifications

    50 KG/Drum
    120 KG/Drum
    1000 KG/Drum
  • Acid value

    1.8 mg KOH/g

  • Volatile

    0.6 %,105℃

  • TDS/MSDS:

    TDS MSDS

Anda boleh menghantar keperluan dan cadangan kepada kami.

We value your requirements and recommendations very much. If you have any questions concerning our services, don't hesitate to ask. Our knowledgeable Rallychem engineers are happy to assist you!

* Nama Syarikat

* Nama

Telefon

* E-mel

* Dari industri mana

Permohonan Industri Lain Bateri Litium Tenaga Baru Pemprosesan logam Buah-buahan/Benih Penandaan peleburan panas Pengubahsuaian asfalt Lem Bantuan Pelapisan dan Ink Bahan Pembantu Tekstil Pengubahsuaian Plastik Kejuruteraan Masterbatch Warna dan Pengisi Pemprosesan CPVC Pemprosesan PVC

Apa yang anda perlukan

WhatsApp

Untuk pertanyaan sila hubungi

Rallychem dengan sukacita akan membantu anda!

+86 13456396233