Our advantages

  • Performance advantage

    Improved hand-folding, compression performance, and good gloss

    Polyester homopolymer replaces CPE, offering better toughness and meeting the standard for 5-degree hand folding

    Improve pressure resistance to meet national standards

    High-speed extrusion, smooth surface, and excellent gloss

  • Cost advantage

    Reduces both formula and overall costs

    Increase production capacity and optimize extrusion speed. From 12-14 m/min to 16-20 m/min

    Heavy calcium can be used without compromising performance and gloss, optimizing cost

    Reduces precipitation and greatly prolongs startup time

    Improved yield

  • Production advantage

    Precipitation reduction

    Extend start-up time

    Continuous stability

    Multi-machine adaptation

Frequently Asked Questions

  • How do you keep output stable at speed and cut plateout?

    +

    Go with a polyester wax + polyester homopolymer combo tuned for molecular weight and low volatility. Dial in internal/external ratios and reduce the total lube. You’ll stretch run time and clean less, across multiple machines.

  • Struggling with the 5°C cold bend?

    +

    Swap CPE for polyester homopolymer to build those fine “energy-absorbing” phases. Combine with the right lubrication and toughening, and you’ll pass the 5°C hand-bend while keeping surface and dimensions steady.

  • Heavy CaCO3 dragging gloss and toughness down?

    +

    · Choose the right particle size and surface treatment.

    · Use polar polyester wax to improve dispersion.

    · Add polyester homopolymer to get toughness back.

    Result: cost down, glossy finish, no fuzz, and solid mechanics.

Rallychem will provide you with professional consulting services, PVC/CPVC customized solution and products including wax additives, wax emulsions, micropolymers customized production,etc. Welcome to contact us.

Contact Us
WhatsApp
WhatsApp QR Code

WhatsApp

Phone

For Inquiries Please Call

Rallychem Will Be Happy To Assist You!

Phone

+86 13456396233

Email
Back to Top
Submit Inquiry