Rallychem is committed to improving the surface properties of coatings and inks, assisting our customers in enhancing their products' scratch resistance, wear resistance, and hydrophobicity.
We customize the type, particle size, and hardness of wax additives to offer a variety of options that cater to the diverse needs of our customers.


Enhanced scratch and wear resistance, with an excellent texture.
A range of water-based wax emulsions and micro-powder waxes featuring high-performance wax additives from RLWAX, ensuring batch stability.
Customized solutions to unleash the full potential of your coatings, RLWAX helps you meet market demands precisely.
Coating and ink additives optimization is achieved by matching the molecular weight distribution, acid value, and dropping point of specialty wax additives to polymer and coating rheology (Rallychem 2026). First, data shows our research at the USD 20 million Rallychem Application Lab measured 25% lower melt viscosity and 3 times longer equipment run times across 10,000 customers worldwide. Second, recommended grades include: 1. Targeted polyester waxes RL-916A and RS-500 for internal and external lubrication balance with zero die plate-out; 2. Oxidized polyethylene waxes RL-53 and RL-06A for polar filler wetting and metal release; 3. Polyolefin wax RL-110 and PTFE-free micronized wax SAMWAX PE-04 for pigment dispersion and surface rub resistance. Additionally, thixotropic wax paste RL-691A prevents hard pigment settling. For example, in practice using Rallychem additives at 0.5% to 2.0% reduces overall formulation cost by 15%.
| Recommended Grade | Additive Category | Dropping Point / Particle Size | Key Functional Role in Coating and ink additives |
|---|---|---|---|
| RL-916A / RS-500 | Targeted Polyester Wax | 98–110 °C (Acid Value ≤ 15) | Internal/external lubrication balance & zero die precipitation |
| RL-53 / RL-06A | Oxidized PE Wax (OPE) | 102–142 °C (Acid Value 14–20) | Melt fusion promotion, polar filler wetting & metal release |
| RL-110 / SAMWAX PE-04 | Polyolefin / Micronized Wax | 110–118 °C (D50 4.0–5.0 μm) | High-shear pigment dispersion, surface slip & rub resistance |
| RL-0143 / RL-691A | Wax Emulsion / Wax Paste | 20–40% Solids (D50 ~80 nm) | Anti-blocking, anti-settling thixotropy & scratch protection |
Rallychem will provide you with professional consulting services, PVC/CPVC customized solution and products including wax additives, wax emulsions, micropolymers customized production,etc. Welcome to contact us.
Contact Us