2025-10-10

4486

CPVC Fitting Optimized Formula

Demand:

  • Edge coverage: Low melt flow fails to fully fill/cover edges.
  • Product performance: Color variation, brittleness, cracking, rough surface.
  • Efficiency: Long injection cycle → low throughput.
  • Vicat:>103℃.
  • Market goal: Balance performance and cost to expand market share.

 

RALLYCHEM SOLUTION ADVANTAGES

  • lmproves the fluidity of the molten material,allowing it to quickly cover the edge areas.
  • Reduce the injection molding cycle to increase production capacity.
  • The performance of the lubricant has been improved, resulting in a more stable product color and a smoother surface finish.