PVC electrical conduit application solution

Demand:

  • Simultaneously meets compression and 5°C low-temperature bend requirements
  • High capacity, fast production speed
  • Cost-competitive formulation

Problem:

  • Compression, hand-bend, and low- temperature performance cannot be satisfied simultaneously
  • Production speed limited to only 10-12 m/min
  • Non-continuous stable production,narrow processing range
  • High material costs

 

Root Cause Analysis:

  • Formulation trade-off conflict: Tuned stiff for compression, but needs toughness for hand- bend and low- temperature bending. The balance is off, so all three can’t be met at once.
  • Narrow processing window: Thermal stability and fusion control are weak; once speed increases, the process becomes unstable, capping the line at 10-12 m/min.
  • High cost: Expensive package plus slow runs and more scrap drive up cost per meter.

PVC-U Irrigation Pipe Enhancement - Rallychem Polymer Additives PVC-U Irrigation Pipe Enhancement - Rallychem Polymer Additives

WhatsApp
WhatsApp QR Code

WhatsApp

Phone

For Inquiries Please Call

Rallychem Will Be Happy To Assist You!

Phone

+86 13456396233

Email
Back to Top
Submit Inquiry